Method of improving the selectivity of carbon membranes by chemical carbon vapor deposition
Abstract
A process for manufacturing carbon membranes having controlled pore sizes comprises the steps of: a) causing a stream of a pyrolysable carbon-containing gas to come into contact with a carbon membrane having a pore size and/or distribution larger than the desired pore size and/or distribution; b) raising the ambient temperature of the said membrane to or above the temperatures at which the adsorbed carbon-containing gas pyrolyzes; and c) substantially purging the atmosphere surrounding the membrane from carbon-containing gas.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 32.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A process for manufacturing an asymmetric carbon membrane from symmetric carbon membranes, said symmetric carbon membrane comprising hollow fibers having pores, said carbon membrane having a shell side and a bore side, said process comprising the steps of: (a) causing a stream of pyrolysable carbon-containing gas having a molecular size greater than the pore size of said hollow fibers to come into contact with either said shell side or said bore side of said symmetric carbon membrane and to be adsorbed thereto; (b) raising and maintaining the temperature of said symmetric membrane to or abov
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗