Solution polymerization process for synthesis of styrene-butadiene or styrene-isoprene rubber
Abstract
The subject invention relates to a technique for synthesizing rubbery copolymers of styrene and butadiene and/or isoprene. These rubbers exhibit an excellent combination of properties for utilization in high performance tire tread rubber compounds. The subject invention specifically discloses a process for preparing a styrene-butadiene rubber (SBR) which comprises: copolymerizing from about 30 weight percent to about 55 weight percent styrene and from about 45 weight percent to about 70 weight percent 1,3-butadiene in an alkane solvent, such as hexane, at a temperature which is within the range of about -10° C. to about 150° C. in the presence of (a) an alkali metal alkoxide, and (b) an organolithium compound, wherein the molar ratio of the alkali metal alkoxide to the organolithium compound is within the range of about 0.01:1 to about 1:1. The subject invention further discloses a process for preparing a rubbery copolymer of styrene and isoprene having an excellent combination of properties for use in making tire treads by a solution polymerization process which comprises: copolymerizing from about 30 weight percent to about 55 weight percent styrene and from about 45 weight perce
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 26.
Claims (2 — 2 Independent, 0 Dependent)
- Claim 1Independent Claim
A process for preparing a rubbery copolymer of styrene and isoprene having an excellent combination of properties for use in making tire treads by a solution polymerization process which comprises copolymerizing from 35 weight percent to about 50 weight percent styrene and from about 50 weight percent to 65 weight percent isoprene in n-hexane solvent at a temperature which is within the range of about 50° C. to about 80° C. in the presence of (a) a sodium alkoxide and (b) an organolithium compound which is of the formula R--Li wherein R represents a hydrocarbyl radical containing from 1 to abo
- Claim 2Independent Claim
A process for preparing a rubbery polymer having an excellent combination of properties for u
Technical Overview & Description