This invention relates to a process for making metal wire, comprising: (A) forming metal foil; (B) cutting said foil to form at least one strand of metal wire; and (C) shaping said strand of wire to provide said strand with desired cross-sectional shape and size. This process is particularly suitable for making copper wire, especially copper wire having a very thin diameter (e.g., about 0.0002 to about 0.02 inch).

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 25 · Forward citations: 28.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A process for making metal wire, comprising: (A) forming a thin web of metal foil having a thickness of about 0.001 to about 0.05 inch, said metal being selected from the group consisting of copper, gold, silver, tin, chromium, zinc, nickel, platinum, palladium, iron, aluminum, steel, lead, brass, or an alloy of one or more of the foregoing metals; (B) cutting said foil to form at least one strand of wire; and (C) shaping said strand of wire to provide said strand with desired cross-sectional shape and size.

  2. Claim 2Depends on #1

    The process of claim 1 wherein said metal is an alloy selected from the group consisting of copper/zinc, copper/silver, copper/tin/zinc, copper/phosphorus, chromium/molybdenum, nickel/chromium and nickel/phosphorus.

  3. Claim 3Depends on #1

    The process of claim 1 wherein said metal is copper or a copper-based alloy.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • 17447, "High Speed Tinning-Line for Copper Wire", Tin and Its Uses, (59), 4-6 (1963).
  • 17447, High Speed Tinning Line for Copper Wire , Tin and Its Uses, (59), 4 6 (1963).
  • 17448, Makowski et al, "Properties of Electrodeposited Foils for Use in Printed Circuits" Paper from Symposium on Electrodeposited Metals as Materials for Selected Applications. Jan. 1972, pp. 14-31.
  • 17448, Makowski et al, Properties of Electrodeposited Foils for Use in Printed Circuits Paper from Symposium on Electrodeposited Metals as Materials for Selected Applications. Jan. 1972, pp. 14 31.
  • 24051, Coppertron, "An Installation For And Method Of Electrolytic Production Of Copper Foil", British Patent 1,588,681 (Apr. 29, 1981).