Abstract

Elastomers exhibiting decreased demold times and improved green strength are prepared by reacting a di- or polyisocyanate with a monodisperse polyoxypropylene diol having ultra-low unsaturation, and preferably prepared by the double metal cyanide.t-butyl alcohol catalyzed polymerization of propylene oxide. Further improved demold times and elevated elastomer physical properties are made possible by the use of multidisperse polyoxyalkylene polyether polyol blends having an overall unsaturation of less than 0.010 meq/g and a polydispersity of about 1.4 or greater.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 15 · Forward citations: 45.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for the improvement of green strength and demold time of polyurethane elastomers prepared by the reaction of an isocyanate component with a polyoxyalkylene polyol and one or more chain extenders, comprising: selecting as said polyoxyalkylene polyol a polyoxyalkylene polyol component having an unsaturation of less than 0.010 meq/g, a polydispersity of 1.4 or greater, and comprising a polyoxypropylene polyol component having an unsaturation of less than 0.010 meq/g, said polyoxyalkylene polyol component having an average equivalent weight of from 1000 Da to about 8000 Da; wherein when

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 45 total)

PatentTitleYearCitations
US 7,309,753 B2Process for the preparation of moisture-curable, polyether urethanes with terminal cyclic urea reactive silane groups20077
US 2007078234 A1Composition for producing polyurea coatings—2
US 5,965,778 APolyurethane elastomers having improved green strength and demold time, and polyoxyalkylene polyols suitable for their preparation199917
WO 2006/055330 A3Cross-linked thermoplastic polyurethane/polyurea and method of making same—0
US 6,884,852 B1Polyurethane and preparation containing polyurethane200564
US 2004251571 A1High performance microcellular foam and manufacturing method and apparatus thereof—2
US 2005027096 A1Polyurethane elastomers having improved physical properties and a process for the production thereof—1
US 2006135637 A1Phthalic anhydride based polyester-ether polyols and double metal cyanide catalyst system for preparing same—4
US 6,884,824 B2Process for preparing an elastomer200517
US 2003176617 A1High performance sealant formulations based on MDI prepolymers—14
US 6,733,707 B1High performance microcellular foam and manufacturing method apparatus thereof20047
US 10,131,759 B2Polyurethane foam and process for producing same20180
US 6,486,268 B2Sealants containing multimodal polymer blends20027
WO 2006/060273 A3Phthalic anhydride based polyester-ether polyols and double metal cyanide catalyst system for preparing same—0
CN 111,518,259 BHigh-resilience polyurethane microporous elastomer and preparation method and application thereof20220

References Cited — Backward Prior Art (15)

PatentTitleYearCitations
US 4,239,879 AThermoplastic polyurethane prepared from a poly-1,2-propylene ether glycol, a low molecular weight glycol and 2,4-tolylene diisocyanate198023
US 5,096,993 AThermoplastic polyurethane elastomers and polyurea elastomers made using low unsaturation level polyols prepared with double metal cyanide catalysts1992113
US 5,100,922 AMethod for producing a molded product of integral-skin polyurethane foam199240
US 5,100,997 APreparation of elastomers using high molecular weight polyols or polyamines, said polyols prepared using a double metal cyanide complex catalyst199270
US 5,106,874 AProcess for preparing elastomeric polyurethane or polyurethane-urea polymers, and polyurethanes so prepared199280
US 5,116,931 AThermoset polyurethane elastomers and polyurea elastomers made using high functionality, low unsaturation level polyols prepared with double metal cyanide catalysts199277
US 5,124,425 ACurable polyurethane composition excellent in flexibility199222
US 5,158,922 AProcess for preparing metal cyanide complex catalyst1992786
US 5,185,420 AThermoplastic polyurethane elastomers and polyurea elastomers made using low unsaturation level polyols prepared with double metal cyanide catalysts199396
US 5,300,535 AMethod for producing polyurethane flexible foam199435
US 5,470,813 ADouble metal cyanide complex catalysts1995758
US 5,482,908 AHighly active double metal cyanide catalysts1996454
US 5,496,496 AProcess for producing polyurethane elastomers199634
US 5,545,601 APolyether-containing double metal cyanide catalysts1996159
US 5,589,431 ADouble metal cyanide complex catalysts199638

Non-Patent Literature (4)

  • C. P. Smith et al., "Thermoplastic Polyurethane Elastomers Made From High Molecular Weight Poly-L™ Polyols", Polyurethane World Congress 1991, Sep. 24-26, 1991, pp. 313-318.
  • C. P. Smith et al., Thermoplastic Polyurethane Elastomers Made From High Molecular Weight Poly L Polyols , Polyurethane World Congress 1991, Sep. 24 26, 1991, pp. 313 318.
  • J. W. Reisch, et al., "Polyurethane Sealants and Cast Elastomers with Superior Physical Properties", 33rd Annual Polyurethane Marketing Conference, Sep. 30-Oct. 3, 1999, pp. 368-374.
  • J. W. Reisch, et al., Polyurethane Sealants and Cast Elastomers with Superior Physical Properties , 33rd Annual Polyurethane Marketing Conference, Sep. 30 Oct. 3, 1999, pp. 368 374.