Patents
US 5,665,291 A#13767366 Most CitedExpiredUnited States (USPTO)Utility

Method for producing high density sintered silicon nitride(Si3 N4)

8Forward Citations (#13767366 Global)
0.3/yrCitation Velocity (#27170182 Global)
1.61Citation PageRank (#20555204 Global)
6Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

The specification describes a method for producing high density sintered silicon nitride (Si 3 N 4 ) having a relative density of at least 98%. In a first step, silicon nitride powder is compacted into a desired shape. It is then pre-sintered in a second step, generally, under normal pressure to obtain a presintered body having a relative density of at least 92%. In a third step, the presintered body is subjected to a hot isostatic pressing (HIP) in an inert gas atmosphere of 1500°-2100° C. and of nitrogen gas partial pressure of at least 500 atm. Since the presintering does not require any capsule, it is possible to produce high density sintered Si 3 N 4 of complex configurations. As a sintering aid, Y 2 O 3 --Al 2 O 3 --MgO system sintering aid is particularly effective. To improve the strength of sintered Si 3 N 4 , it is effective to add a heat treatment step after the HIP and maintain the temperature of the sintered Si 3 N 4 above 500° C. for a while. Between the second and third steps, the temperature of the presintered body is preferably maintained above 500° C. These temperature controls are effective not only to improve the strength of sintered Si 3 N 4 but also to save th

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 8.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for producing high density sintered silicon nitride (Si 3 N 4 ) having a relative density of at least 98%, said method comprising: forming silicon nitride powder into a desired shape to obtain a silicon nitride green compact; presintering said green compact under a nitrogen gas atmosphere ranging in pressure from 1 to 30 atmospheres at a temperature of 1500°-1600° C. for 50-200 minutes into a presintered Si 3 N 4 body whose α--Si 3 N 4 content ranges from 80-20% and whose β--Si 3 N 4 content ranges from 20-80% and which has a relative density of at least 92%; removing the p

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • Abstract of German Patent 2621523.
  • Kobe Steel, Ltd., No. 313011, Hot and Cold Isostatic Pressing Equipment, pp. 1 10.
  • Kobe Steel, Ltd., No. 313011, Hot and Cold Isostatic Pressing Equipment, pp. 1-10.
  • Kobe Steel, Ltd., No. 428090, Hot Isostatic Press, pp.1 6.
  • Kobe Steel, Ltd., No. 428090, Hot Isostatic Press, pp.1-6.