Process for direct production of low acetaldehyde packaging material
Abstract
Process for direct production of shaped packaging material made of thermoplastic polyesters with no effect on the taste of foods packaged in them, where the diol component of the polyester consists of at least 70 wt % ethylene glycol, and the polyester is produced in the presence of the usual catalysts plus additional cobalt or cobalt and manganese compounds and phosphorus compounds. An inert gas is introduced into the polyester melt and distributed uniformly in the melt immediately after its discharge from the polycondensation reactor, 0.05 to 1.0 wt % of an amide compound with a low volatility is added to the polyester melt directly next to the gas inlet. Finally, the polyester melt is subjected to a vacuum degassing immediately before the shaping apparatus and the melt is sent directly to the shaping apparatus within a maximum of 30 minutes after its discharge from the reactor at a maximum temperature of 35° C. above the crystallite melting point of the polyester.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 19 · Forward citations: 71.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
Process for the reduction of the free aldehyde content in a polyester melt during production of shaped polyester food packaging material which does not affect taste of the food, the steps of which are carried out as polyester in the melt phase flows directly from a poly-condensation reactor to a shaping apparatus, said polyester having at least 70 wt % ethylene glycol units based on the total diol units, said process comprising (a) providing a polyester melt which contains, in addition to conventional reaction catalysts, an added 5-120 ppm of a) cobalt or b) cobalt and manganese in a molar rat
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗