Tetracalcium phosphate-based materials and processes for their preparation
Abstract
The invention provides (i) a process for preparing tetracalcium phosphate particles, the process comprising the steps of (1) sintering or fusing a powder mixture at a temperature of not lower than 1,400° C., the mixture comprising a powder of calcium source and a powder of phosphorus source in a Ca/P molar ratio of 2/1, and about 0.005 to about 5 parts of an aluminum compound, calculated as Al 2 O 3 , per 100 parts of tetracalcium phosphate to be produced in terms of the theoretical amount, and (2) finely dividing the obtained product; (ii) tetracalcium phosphate particles prepared by said process; (iii) apatite-coated tetracalcium phosphate particles; (iv) a process for preparing the apatite-coated tetracalcium phosphate particles; (v) a tetracalcium phosphate-based setting composition; (vi) a composition for forming a hardening material using coated tetracalcium phosphate particles and an acidic aqueous solution; and (vii) the composition as defined in (vi) in which the acidic aqueous solution can satisfy the concentration relationships as represented below: (a) 25%≦citric acid≦50% (b) 30%≦citric acid+phosphoric acid≦70% (c) 10%≦citric acid-phosphoric acid≦50%.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 89.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A process for preparing tetracalcium phosphate particles coated with apatite, the process comprising contacting tetracalcium phosphate particles with water having a pH of at least 8 for a time sufficient to form a coating of apatite on the outer surface of the tetracalcium phosphate particles.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗