Patents
US 5,651,995 A#531635 Most CitedExpiredUnited States (USPTO)Utility

Highly saturated nitrile rubber, process for producing same, vulcanizable rubber composition, aqueous emulsion and adhesive composition

67Forward Citations (#531635 Global)
2.3/yrCitation Velocity (#1546157 Global)
12.62Citation PageRank (#720750 Global)
25Prior Art Cited
3Claims (2 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A nitrile group-containing highly saturated copolymer rubber which is a product obtained by hydrogenating the conjugated diene portion of an unsaturated nitrile-conjugated diene copolymer. The highly saturated copolymer rubber has an alkylthio group having 12 to 16 carbon atoms, which include at least three tertiary carbon atoms, and having a sulfur atom which is directly bound to at least one of the tertiary carbon atom, and the highly saturated copolymer rubber further has a Mooney viscosity of 15 to 200 and an iodine value not larger than 80. The highly saturated copolymer rubber is produced copolymerizing an unsaturated nitrile, a conjugated diene and an optional copolymerizable monomer by using as a molecular weight modifier an alkylthiol compound having 12 to 16 carbon atoms, which include at least three tertiary carbon atoms, and having a sulfur atom which is directly bound to at least one of the tertiary carbon atoms; and then, hydrogenating the thus-obtained copolymer. The highly saturated copolymer rubber exhibits a high-rate vulcanizability when vulcanized with a sulfur-containing vulcanizer.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 25 · Forward citations: 67.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A nitrile group-containing highly saturated copolymer rubber which is a product obtained by hydrogenating the conjugated diene portion of an unsaturated nitrile-conjugated diene copolymer; said highly saturated copolymer rubber having an alkylthio group having 12 to 16 carbon atoms, which include at least three tertiary carbon atoms, and having a sulfur atom which is directly bound to at least one of the tertiary carbon atoms; and said highly saturated copolymer rubber further having a Mooney viscosity of 15 to 200 and an iodine value not larger than 80.

  2. Claim 2Depends on #1

    A nitrile group-containing highly saturated copolymer rubber as claimed in claim 1, wherein said highly saturated copolymer rubber has at least 0.03 mole, per 100 moles of the monomeric units constituting the molecule, of said alkylthio group.

  3. Claim 3Independent Claim

    A nitrile gr

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (4)

  • J. Soc. Rub. Ind., Jp, vol. 59, No. 4, pp. 210 214, 1986.
  • J. Soc. Rub. Ind., Jp, vol. 59, No. 4, pp. 210-214, 1986.
  • N. Asada et al., Rub. Chem. & Tech., Composition Distribution of Acrylonitrile Butadiene . . . , vol. 63, No. 2, pp. 181 190.
  • N. Asada et al., Rub. Chem. & Tech., Composition Distribution of Acrylonitrile-Butadiene . . . , vol. 63, No. 2, pp. 181-190.