Process for producing silicon carbide
Abstract
Disclosed is a process for producing silicon carbide. The process includes the steps of (1) mixing β-resin extracted from coal-tar pitch with α-resin and silica gel; (2) after being dried, grinding the mixture to powder; (3) heating the powder in an atmosphere of nitrogen with a temperature in the range from 300° C. to 480° C. until mesophase is cultured; and (4) proceeding the heat treatment with a higher temperature in the range from 900° C. to 1200° C. for a period in the range from 2 to 7 hours. By the process, the production of silicon carbide can be carried out at low temperatures so that it is cost-effective in energy consumption.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 3.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A process for producing silicon carbide, comprising the following steps of: (1) mixing β-resin extracted from coal-tar pitch with α-resin and silica gel to form a mixture; (2) drying the mixture and grinding the dried mixture to powder; (3) heating the powder in an atmosphere of nitrogen at a temperature in the range from 300° C. to 480° C. until a mesophase is cultured; and (4) heating the powder at a temperature in the range from 900° C. to 1200° C. for a period in the range from 2 to 7 hours.
- Claim 2Depends on #1
A process as claimed in claim 1, wherein the percentage by weight of α-resin used in said Step (1) is 1 wt %-10 wt %.
- Claim 3Depends on #2
A process as claimed in claim 2, wherein the percentage by weight of α-resin used in said Step (1) is 1 wt %-5 wt %.