Patents
US 5,650,106 A#1659519 Most CitedExpiredUnited States (USPTO)Utility

Extruded foams having a monovinyl aromatic polymer with a broad molecular weight distribution

36Forward Citations (#1659519 Global)
1.2/yrCitation Velocity (#4859677 Global)
7.12Citation PageRank (#1861292 Global)
4Prior Art Cited
2Claims (2 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Disclosed is an extruded, linear, bimodal monovinyl aromatic polymer foam having a weight average molecular weight of from about 100,000 to about 200,000, greater than 5 percent by weight of its polymer chains having a weight average molecular weight of 500,000 to 1,000,000, and less than 5 percent by weight of its polymer chains having a weight average molecular weight of greater than 1,000,000. Use of the polymer enables process pressure drop to be significantly reduced and allows the formation of a foam of lower density and larger cross-section. Further disclosed is a process for making the extruded foam.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 36.

Claims (2 — 2 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for making an extruded, monovinyl aromatic polymer foam, comprising: a) heating to form a melt polymer material a polymer material comprising greater than 50 percent by weight of monovinyl aromatic monomeric units and comprising a monovinyl aromatic polymer having: i) a weight average molecular weight of about 100,000 to about 250,000; and ii) greater than 5 percent by weight of its polymer chains of a weight average molecular weight of 500,000 to 1,000,000 and less than 5 percent by weight of its polymer chain of a weight average molecular weight or greater than 1,000,000; b)

  2. Claim 2Independent Claim

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗