Building material with increased strength
Abstract
In order to be able to produce formed elements or building elements with a significantly increased strength with a building material or structural material, it is suggested to provide the material with a largely uniform fine pore structure or a microcellular structure. These fine pores preferably have a diameter in the range of approx. 0.01μ to approx. 5μ and are self-contained. The material contains a reactive binding agent or a reactive matrix material, which can be a cement/water mixture or also a synthetic resin, for example polyurethane, epoxy resin, etc.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 18.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A porous hydrate cement product having a generally uniform distribution of fine pores after mix-up wherein said cement product is obtained by a process of mixing a cement composition in a high turbulence mixer, which mixes the cement composition at a speed of approximately 1500 revolutions per minute, for a sufficient period of time wherein after mix-up said pores in said cement product have a diameter ranging between about 0.01 micrometers and about 5 micrometers.
- Claim 2Depends on #1
The composition of claim 1 wherein aggregates are added to said composition, said aggregates being selected from the group consisting of sand, gravel, and lightweight filler material.
- Claim 3Depends on #2
The composition of claim 2 wherein said lightweight filler material has a density of less than 0.1 gm/cm 3 is selected from the group consisting of glass fibers, polystyrene
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗