Patents
US 5,628,045 A#8175528 Most CitedExpiredUnited States (USPTO)Utility

Process and device for producing sintered parts

12Forward Citations (#8175528 Global)
0.4/yrCitation Velocity (#19476670 Global)
2.87Citation PageRank (#8117026 Global)
5Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A process for producing sintered parts with high wear resistance and good dynamic strength properties from formed bodies, which have been pressed as green parts from a completely-alloyed air-hardened heat-treatment steel powder with a carbon content of at least 0.3% added in the form of graphite. The process includes sintering the parts under protective gas at a sintering temperature of at least 1000° C. and subsequent cooling. The sintered parts are cooled immediately after sintering from the sintering temperature to a first holding temperature in the range of Ar 3 to a maximum of 150° C. above Ar 3 and are held for a first holding period of 5 to 25 minutes at this temperature (austenitizing phase). Immediately after this, the sintered parts are cooled in accelerated fashion to a second holding temperature by convective gas cooling and are held at this temperature for a second holding period. The second holding temperature lies in a temperature range in which a bainitic structure forms and is of such a length that a bainitic structure portion of at least 50% is established. The sintered parts are then cooled to room temperature.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 12.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for producing a sintered part with high wear resistance and good dynamic strength properties from a formed body which has been pressed as a green part from a completely-alloyed air-hardened heat-treatment steel powder with a carbon content of at least 0.3% added as graphite, the process comprising the steps of: sintering the part under protective gas at a sintering temperature of at least 1000° C.; immediately cooling, the sintered part from the sintered temperature to a first holding temperature in a range of Ar 3 to a maximum of 150° C. above Ar 3 and holding the part at the fi

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗