Abstract

A method for passivating diamond films to substantially prevent them from oxidizing at temperatures up to 800° C. in an oxygen atmosphere. The method involves depositing one or more passivating layers over the diamond film wherein one of the layers is nitride and the other layer is quartz. The passivation technique is directly applicable to diamond sensor pressure transducers and enable them to operate at temperatures above 800° C. in oxygen environments. The passivation technique also provides an economical and simple method for patterning diamond films.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 9 · Forward citations: 11.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for preventing a diamond film coated on a substrate from oxidizing at temperatures above 800° C. in an oxygen atmosphere, comprising the steps of: placing said diamond film coated on the substrate into a reactor set a first temperature which is below a temperature at which diamond oxidizes; evacuating said reactor set at the first temperature remove all oxygen therefrom; raising said reactor to a second temperature; and depositing a passivation layer over said diamond film at the second temperature, whereby said passivation layer prevents said diamond film from oxidizing at temp

  2. Claim 2Depends on #1

    The method according to claim 1, wherein said first temperature is approximately 550° C.

  3. Claim 3Depends on #1

    The method according to claim 1, wherein said reactor is evacuated down to 1 m

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • D.R. Wur, J.L. Davidson, W.P. Kang, D.L. Kinser, IEEE J Microelectromech. Syst. 4, 1 pp. 34 41, (1995).
  • D.R. Wur, J.L. Davidson, W.P. Kang, D.L. Kinser, IEEE J Microelectromech. Syst. 4, 1 pp. 34-41, (1995).
  • J.L. Davidson, J.S. Shor, D.R. Wur, and A.D. Kurtz, J. Electrochem. Soc., 141, 12, pp. 3522 3525, (1994).
  • J.L. Davidson, J.S. Shor, D.R. Wur, and A.D. Kurtz, J. Electrochem. Soc., 141, 12, pp. 3522-3525, (1994).
  • J.L. Davidson, R. Ramasham, C. Ellis, J. Electrochem. Soc., 137, 10 (1990) pp. 3206 3210.