Process for the preparation of Quinacridone pigments

19Forward Citations (#4632727 Global)
0.7/yrCitation Velocity (#12145360 Global)
2.57Citation PageRank (#9702309 Global)
26Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

Pigments, mixed-crystal pigments or pigment preparations based on linear, unsubstituted or substituted quinacridones are prepared advantageously by initially wet-milling the coarsely crystalline crude pigments in a liquid aqueous, aqueous-organic or organic medium in a stirred ball mill which is operated at a power density of more than 2.5 kW per liter of milling space and a peripheral stirrer speed of more than 12 m/s under the action of grinding media having a diameter of less than or equal to 0.9 mm, until the desired degree of fine division is reached, and then isolating the resulting pigment in a conventional manner, or subjecting the resulting prepigment to solvent treatment at a temperature of from 50° to 200° C. and then isolating the pigment in a conventional manner.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 26 · Forward citations: 19.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A process for the preparation of a pigment, mixed-crystal pigment or pigment preparation based on linear, unsubstituted quinacridones of β-phase or γ-phase, or substituted, linear quinacridones, which comprises: initially wet-milling a coarsely crystalline crude pigment in a liquid aqueous, aqueous-organic or organic medium in a stirred ball mill which is operated at a power density of more than 2.5 kW per liter of milling space and a peripheral stirrer speed of more than 12 m/s under the action of grinding media having a diameter of less than or equal to 0.9 mm, until fine division is reached

  2. Claim 2Depends on #1

    The process as claimed in claim 1, wherein grinding media having a diameter of from 0.2 to 0.9 mm are employed.

  3. Claim 3Depends on #1

    The process as claimed in claim 1, wherein grinding media having a dia

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (2)

  • European Search Report No. 95100786.3 Apr. 19, 1995.
  • European Search Report No. 95100786.3 -Apr. 19, 1995.