Method for forming TiN film and TiN film/thin TiSi2 film, and method for fabricating semiconductor element utilizing the same
Abstract
A method for forming a fine-textured titanium nitride film and fine-textured titanium nitride/thin titanium silicide films, and methods for fabricating semiconductor elements utilizing the same are disclosed. A thin titanium silicide film and a fine-textured nitride film are formed on a semiconductor substrate through depositing a titanium film containing nitrogen on the semiconductor substrate by sputtering a titanium target having a titanium nitride film formed thereon and quenching. A bit line of a COB DRAM element may be formed of tungsten, and a tungsten bit line having good contact characteristics and preserved barrier characteristics can be formed since the fine-textured titanium nitride/thin titanium silicide films may serve as a barrier preventing the tungsten from diffusing at high temperature during subsequent capacitor forming processes. The fine-textured titanium nitride/thin titanium silicide films may be applied to an aluminum wiring, and the titanium silicide formed at the contact part may improve the contact characteristics, and TiAl 3 formed between the titanium nitride film and the aluminum wiring may improve the electromigration characteristics of the metal wiri
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 2.
Claims (3)
- Claim 1Independent Claim
A method of forming a titanium nitride film comprising the steps of: preparing a titanium target; forming a titanium nitride film on the titanium target; forming an oxide film on a semiconductor substrate; depositing a titanium film containing nitrogen on the oxide film by sputtering under an argon atmosphere the target having the titanium nitride film formed thereon; and forming a nitride film on the oxide film by heat-treating the titanium film.
- Claim 2Depends on #1
The method of claim 1, wherein the titanium film is subjected to heat-treatment for one to three times.
- Claim 3Depends on #1
The method of claim 1, wherein the heat-treatment process is carried out for about 40 seconds at a temperature of about 500° C. and for about 30 seconds at a temperature of about 800° C.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (2 of 2 total)
References Cited — Backward Prior Art (11)
| Patent | Title | Year | Citations |
|---|---|---|---|
| EP 4,180,596 B1 | Transmission structure of smart lock cylinder and smart lock | 2023 | 0 |