Patents
US 5,594,930 A#4555418 Most CitedExpiredUnited States (USPTO)Utility

Brazeable aluminum material and a method of producing same

19Forward Citations (#4555418 Global)
0.7/yrCitation Velocity (#12143309 Global)
3.22Citation PageRank (#6772028 Global)
7Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A brazeable aluminum material is composed of an aluminum core and a brazing agent layer consisting of a brazing agent thermally sprayed onto covering a surface of the core. A number of unmolten minute particles of the brazing agent are present in the brazing agent layer, which contains at least an aluminum-silicon alloy and/or a mixture of aluminum and silicon. Characteristic features of a method of producing the brazeable aluminum material are the steps of: preparing a powder composed of minute particles; and thermally spraying the powder onto the aluminum core in such a state that only a surface of each minute particle is molten, with a pith of the particle remaining unmolten. The powder is an Al-Si alloy and/or a mixture of Al powder and Si powder.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 19.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of producing a brazeable aluminum material wherein a brazing agent layer is thermally sprayed onto an aluminum core of the brazeable aluminum material, the method comprising the steps of: preparing a powder composed of minute particles to be thermally sprayed to form the brazing agent layer; and then thermally spraying the powder onto the aluminum core in such a state that only a surface of each of substantially all the minute particles is molten, with a pith of each particle remaining unmolten.

  2. Claim 2Depends on #1

    The method as defined in claim 1, wherein the powder comprises an Al-Si alloy such that an average Si content in the brazing agent layer is from about 5 to about 40% by weight.

  3. Claim 3Depends on #2

    The method as defined in claim 2, wherein the average Si content in the brazing layer is from about 8 to about 13% by weight.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (2)

  • B. Wielage et al. "Hochtemperaturloten von X 5 CrNi 18 10 und NiCr 20 TiAl bei durch thermisches Spritzen aufgebrachten Loten," Schweissen Und Schneiden, vol. 42, No. 5, May 1990, pp. 228-231 (translation included).
  • B. Wielage et al. Hochtemperaturloten von X 5 CrNi 18 10 und NiCr 20 TiAl bei durch thermisches Spritzen aufgebrachten Loten, Schweissen Und Schneiden, vol. 42, No. 5, May 1990, pp. 228 231 (translation included).