Glass bubbles for use as fillers in printed circuit board
Abstract
Glass bubbles for use as fillers in a plastic resin substrate of an electrical printed circuit board are light in weight, low in density, and small in alkali amount leached sufficiently to insure electrical insulation resistance of the substrate, and consist essentially of, by weight, SiO2 40.0-60.0%, Al2O3 5.0-22.0%, B2O3 1.0-15.0%, CaO 10.0-30.0%, BaO 0-15.0%, MgO 0-10.0%, ZnO 0-10.0%, SrO 0-10.0%, Na2O+K2O+Li2 O 0-1.9%, As2O3+Sb2O3 0-1.54, V2O5 0-10.0%, TiO2 0-10.0%, and SO3 0.05-1.7%.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 9.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
Glass bubbles for use in fillers for plastic resin articles and made by heating bubble-forming powders of a composition containing SO 3 , said glass bubbles consisting essentially of, by weight, SiO 2 40.0-60.0%, Al 2 O 3 5.0-22.0%, B 2 O 3 1.0-15.0%, CaO 10.0-30.0%, BaO 0-15.0%, MgO 0-10.0%, ZnO 0-10.0%, SrO 0-10.0%, Na 2 O+K 2 O+Li 2 O 0-1.9%, As 2 O 3 +Sb 2 O 3 0-1.5%, V 2 O 5 0-10.0%, TiO 2 0-10.0%, and SO 3 0.05-1.7%.
- Claim 2Depends on #1
Glass bubbles as claimed in claim 1, which have diameters of 45 μm or less and relative density of 0.4-1.4 g/cm 3 .
- Claim 3Depends on #1
Glass bubbles as claimed in claim 1, wherein SiO 2 is 42.0-58.0%, Al 2 O 3 is 5.0-20.0%, B 2 O 3 is 2.0-12.0%, CaO is 18.0-27.0%, BaO is 0.1-13.0%, MgO is 0-6.0%, ZnO is 0-6.0%, SrO is 0-6.0%, Na 2 O+K 2 O+Li 2 O is 0-1.9%, As 2 O 3 +Sb 2 O 3 is