Patents
US 5,587,325 A#7508012 Most CitedExpiredUnited States (USPTO)Utility

Method of preparing antimony doped semiconductor with intrinsic gettering

13Forward Citations (#7508012 Global)
0.4/yrCitation Velocity (#18619349 Global)
2.70Citation PageRank (#8957967 Global)
11Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A method of preparing semiconductor wafers with intrinsic gettering capability, comprises the steps of: carrying out a high temperature wet oxidation on a doped semiconductor wafer for between about 20 to 60 minutes to form an initial oxidation layer; heating said wafer at a moderate temperature in an inert atmosphere for about 1 to 4 hours to initiate formation of crystal nuclei; ramping up the temperature in said inert atmosphere to a temperature of at least about 850° C. at a rate of about 1°-10° C./min.; and subsequently carrying out well diffusion on the wafer at a temperature of at least about 1000° C.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 13.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    1. A method of preparing a antimony-doped semiconductor wafer with intrinsic gettering capability, comprising consecutively carrying out the steps of: a) exposing the antimony doped wafer to a wet oxidizing atmosphere at a steady temperature above about 1000° C. for between about 20 to 60 minutes to form an oxidation layer thereon; b) immediately after step (a) heating said wafer at a steady temperature of between about 600°-700° C. in an inert atmosphere for about 1 to 4 hours to initiate formation of crystal nuclei in the wafer; c) carrying out a single ramp cycle in said inert atmospher

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗