Patents
US 5,587,203 A#5614575 Most CitedExpiredUnited States (USPTO)Utility

Method for preparing a carbon/carbon composite material

16Forward Citations (#5614575 Global)
0.5/yrCitation Velocity (#14844269 Global)
4.06Citation PageRank (#4656552 Global)
5Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A method for preparing a carbon/carbon composite material which is characterized in that a carbon preform is impregnated with a carbonaceous pitch exhibiting a densification parameter of 0.1 or more, said densification parameter being represented by the following formula (1), and then subjected to an isotactic compression at a pressure higher than the atmospheric pressure but not higher than 10 Kgf/cm 2 and at a sintering temperature of 250° to 3,000° C., thereby densifying the carbon preform: Densification parameter={(Weight of a sintered carbonaceous pitch (hereinafter, referred to simply as a sintered product) to be obtained through a process where a carbonaceous pitch in an open-type container is heated from room temperature up to 1000° C. at a rate of 2° C./min., and then sintered for 2 hours at 1000° C. under isotactic compression of 9.5 Kgf/cm 2 )}/(Weight of a carbonaceous pitch before being sintered)×{(Bulk density of the sintered product in the open-type container)/(True density of the sintered product)}. . . (1).

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 16.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of preparing a carbon/carbon composite material which consists of the steps of 1) impregnating a carbon preform with a carbonaceous pitch, said carbonaceous pitch having a carbon/hydrogen atomic ratio of less than 1.60 and exhibiting a densification parameter of 0.1 or more, said densification parameter being calculated by heating said carbonaceous pitch in an open-type crucible from room temperature up to 1000° C. at a rate of 2° C./min. and then keeping at 1000° C. for two hours whereby said carbonaceous pitch is sintered, said densification parameter being calculated by the formula

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (2)

  • Carbon, vol. 11, pp. 570 574, 1973 E. Fitzer et al, The pryolysis . . . (no mo.).
  • Carbon, vol. 11, pp. 570-574, 1973 E. Fitzer et al, "The pryolysis . . . "(no mo.).