Patents
US 5,583,073 A#803397 Most CitedExpiredUnited States (USPTO)Utility

Method for producing electroless barrier layer and solder bump on chip

54Forward Citations (#803397 Global)
1.8/yrCitation Velocity (#2504645 Global)
10.67Citation PageRank (#953374 Global)
11Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

The present method for producing a barrier layer and a solder bump on a chip includes: a) providing a silicon chip with a bump base; b) forming a metal pad, e.g. an aluminum pad, on the bump base; c) having the metal pad contact with a solution containing about 120˜150 g/l NaOH, 20˜25 g/l ZnO, 1 g/l NaNO 3 and 45˜55 g/l C 4 H 4 KNaO 6 ·4H 2 O to form thereon a zinc layer, and preferably further containing tartaric acid for reducing a dissolving rate of the metal pad.; d) having the zinc layer contact with a deposition solution to deposit thereon an electroless barrier layer, e.g. an electroless Ni-P layer; and e) dipping the resulting silicon chip into a molten solder bath to form a solder bump on the electroless barrier layer. The present invention is a simple process for manufacturing an electroless Ni-P and a solder bump on a chip.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 54.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of producing a barrier layer and a solder bump on a chip comprising: a) providing a silicon chip with a bump base; b) forming a metal pad on said bump base; c) having said metal pad contact with a solution containing about 120-150 grams/liter NaOH, 20-25 grams/liter ZnO, 1 grams/liter NaNO 3 and 45-55 grams/liter C 4 H 4 KNaO 6 ·4H 2 O to form thereon a zinc layer; d) having said zinc layer contact with a deposition solution to deposit thereon an electroless barrier layer; and e) dipping said resulting silicon chip into a molten solder bath to form a solder bump on said e

  2. Claim 2Depends on #1

    The method according to claim 1 further comprising a step b') before said step c) of washing said first metal pad with an alkaline solution.

  3. Claim 3Depends on #2

    The method according to claim 2 wherein said

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (4)

  • K. Wang, K. Chi and A. Rangappan, "Application of Electroless Nickel Plating in the Semiconductor Microcircuit Industry", Plating and Surface Finishing, 70, Jul. 1988.
  • K. Wang, K. Chi and A. Rangappan, Application of Electroless Nickel Plating in the Semiconductor Microcircuit Industry , Plating and Surface Finishing, 70, Jul. 1988.
  • M. Inaba, K. Yamakawa, and N. Iwase, "Solder Bump Formation Using Electroless Plating and Ultrasonic Soldering", IEEE Transactions on Components, Hybrids, and Manufacturing Technology, vol. 13, No. 1, 119, Mar. 1990.
  • M. Inaba, K. Yamakawa, and N. Iwase, Solder Bump Formation Using Electroless Plating and Ultrasonic Soldering , IEEE Transactions on Components, Hybrids, and Manufacturing Technology, vol. 13, No. 1, 119, Mar. 1990.