Patents
US 5,582,879 A#2999515 Most CitedExpiredUnited States (USPTO)Utility

Cluster beam deposition method for manufacturing thin film

25Forward Citations (#2999515 Global)
0.8/yrCitation Velocity (#8668958 Global)
4.73Citation PageRank (#3633006 Global)
11Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

In a method of manufacturing a thin film, evaporated particles are generated by a vapor source and are clustered. The clustered evaporated particles are deposited onto a substrate in a vacuum atmosphere without ionizing the particles. A partial pressure of water in the vacuum atmoshpere is controlled to not more than 5×10 -6 Torr. A temperature of the substrate is maintained to be 150° C. or lower. A film according to this method has a high adhesion characteristics and a high mechanical strength without heating the substrate to a high temperature and without damaging the substrate by ions.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 25.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A thin film manufacturing method comprising the steps of: clustering evaporated particles generated by a vapor source; and depositing the clustered evaporated particles onto a substrate in a vacuum atmosphere without ionizing the particles, wherein a partial pressure of water vapor in the vacuum atmosphere is controlled to not more than 5×10 -6 Torr.

  2. Claim 2Depends on #1

    A method according to claim 1, wherein a temperature of the substrate is maintained to be not exceeding 150° C.

  3. Claim 3Depends on #1

    A method according to claim 1, wherein the substrate consists of a plastic material.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 25 total)

PatentTitleYearCitations
US 6,022,598 AICB method of forming high refractive index films20003
US 6,375,790 B1Adaptive GCIB for smoothing surfaces200266
EP 1,282,161 A4LOW RELATIVE PERMITTIVITY SIO x? FILM, PRODUCTION METHOD, SEMICONDUCTOR DEVICE COMPRISING THE FILM—0
US 7,179,508 B2Conducting polymer films and method of manufacturing the same by surface polymerization using ion-assisted deposition20071
US 8,835,880 B2Charged particle-beam processing using a cluster source20145
US 5,989,990 ATinoxide thin film, preparation thereof, and gas detecting sensor using thereof19996
US 2014319333 A1Apparatus and method relating to an improved mass spectrometer—5
US 6,562,200 B2Thin-film formation system and thin-film formation process200316
CN 108,690,963 AFilm formation device—8
US 11,446,714 B2Processing apparatus and processing method, and gas cluster generating apparatus and gas cluster generating method20220
US 2010025852 A1Semiconductor device and method for manufacturing the same—40
US 10,825,685 B2Method for neutral beam processing based on gas cluster ion beam technology and articles produced thereby20202
US 9,147,568 B2Water cluster ion beam mass spectrometer apparatus and method20150
US 6,761,431 B2Polymer film, polymeric compound for forming the same, method of manufacturing such polymeric compound, liquid-repellency treatment solution using such polymeric compound, surface-modifying method using such treatment solution and surface-modified article20042
US 2002185369 A1Method of forming film by sputtering, optical member, and sputtering apparatus—10