Abstract

Gel-free ethylene/vinyl acetate copolymers with a high content of copolymerized vinyl acetate and a high Mooney viscosity are produced by carrying out the polymerization in solution in the presence of 20 to 45% by weight tert.butanol, based on the reaction solution, at temperatures of 50° to 80° C. and under pressures of 300 to 450 bar using azo compounds in a cascade of stirred reactors with an average residence time of the reaction solution in the reactor cascade of 5 to 9 hours and a conversion of 50 to 70% by weight, based on the vinyl acetate used. The ethylene/vinyl acetate copolymers produced by the process according to the invention may be used for the production of vulcanizates having improved mechanical properties.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 19.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A process of preparing ethylene/vinyl acetate copolymers consisting of producing gel-free ethylene/vinyl acetate copolymers having 30-90% copolymerized vinyl acetate and a Mooney viscosity of 10-80 by polymerizing ethylene and vinyl acetate in a solution which is free of other monomers and which contains 20-45% by weight, based on weight of solution, of tert.-butanol, in the presence of an azo initiator, at temperatures of 50°-80° C. and under pressures of 300 to 450 bar, in a cascade of stirred reactors with an average residence time of the solution in the reactor cascade of 5-9 hours and a c

  2. Claim 2Depends on #1

    The process of claim 1, wherein the polymerized vinyl acetate content is 40-80% by weight and the Mooney viscosity is 20-40.

  3. Claim 3Depends on #1

    The process as claimed in claim 1, wherein