Polyketone yarn and a method of manufacturing same
Abstract
The invention relates to polyketone yarns of which the maximum tangential modulus at an elongation of more than 0.2% is at least 10 N/tex which display both high strength and, if so desired, a high elongation at break. The quality number, which is measured on a single filament out of a bundle of at least about 30 filaments spun simultaneously through one spinneret and given as σ.ε, is higher than 85 mN/tex, preferably higher than 100 mN/tex. The quality number of a yarn spun through one spinneret of one or more holes is higher than 110 mN/tex, preferably higher than 120 mN/tex. The yarns are manufactured by extruding a solution of a linear polymer of alternating ethylene and carbon monoxide units in a resorcinol-containing solvent, after which the solvent is removed with the aid of methanol as coagulant.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 24 · Forward citations: 6.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A yarn comprising a linear polymer of alternating ethylene and carbon monoxide units, wherein the yarn is spun in a single step, the yarn has a maximum tangential modulus, at an elongation of more than 0.2%, of at least 10 N/tex, the yarn has a quality number, according to the formula σ.ε, higher than 85 mN/tex and the yarn comprises at least 30 filaments which are spun simultaneously through one spinneret.
- Claim 2Depends on #1
The yarn of claim 1 wherein the quality number is higher than 100 mN/tex.
- Claim 3Depends on #2
The yarn according to claim 2 wherein the quality number is higher than 120 mN/tex.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗