Patents
US 5,547,902 A#5163599 Most CitedExpiredUnited States (USPTO)Utility

Post hot working process for semiconductors

17Forward Citations (#5163599 Global)
0.6/yrCitation Velocity (#13779928 Global)
4.48Citation PageRank (#3966501 Global)
8Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A post-hot metal deposition process applied to semiconductor wafer manufacturing in order to increase the size of grain structures and improve electromigration resistance in semiconductor devices. A highly ductile metal is first deposited onto a semiconductor substrate having contact points in a partial vacuum. A forge is applied to the substrate--with the highly ductile metal deposited thereon, to form a smooth conductive surface on the substrate, even at the contact points. The forging is done at an appropriate pressure and temperature to perform hot-working of the metal onto the contact points of the substrate. The forge may be used to emboss a conductor image of the highly ductile metal deposited on the substrate. The forging process may be performed by either stamping a surface onto the substrate or by rolling a surface onto the substrate.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 17.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for depositing a ductile metal onto a semiconductor substrate having a plurality of contact openings in order to fill in said contact openings, the method comprising the steps of: a) depositing said ductile metal onto said semiconductor substrate in a partial vacuum environment; b) compressing said ductile metal onto said semiconductor substrate using a forge in a full vacuum environment; and c) cooling said semiconductor substrate with said ductile metal compressed thereon.

  2. Claim 2Depends on #1

    The method recited in claim 1, wherein said ductile metal is Aluminum, and said fixed compression is about 4300 pounds per square inch of said semiconductor substrate.

  3. Claim 3Depends on #1

    The method recited in claim 1, wherein the step a) is performed at a temperature of about 275 degrees Centigrade.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗