Patents
US 5,543,472 A#10492665 Most CitedExpiredUnited States (USPTO)Utility

Concurrent epoxidation and catalyst residue extraction

10Forward Citations (#10492665 Global)
0.3/yrCitation Velocity (#22693316 Global)
2.04Citation PageRank (#14072205 Global)
4Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A process for the concurrent epoxidation of, and catalyst residue extraction from, anionically polymerized diene-containing polymers which have been hydrogenated using a Group VIII metal catalyst, said process comprising: (a) introducing a catalyst residue-containing diene-containing polymer cement into a reactor, (b) heating the polymer cement to a temperature of 25° to 65° C., (c) contacting the polymer cement with a caustic solution, (d) contacting the polymer cement with a peracid solution, (e) mixing the polymer, caustic, and acid at 25° to 65° C. for 1/2 to 3 hours, (f) optionally adding sufficient caustic solution to neutralize excess acid while continuing the mixing, (g) adding sufficient water such that the aqueous/organic phase weight ratio is from 0.2:1 to 1:1 while continuing the mixing, (h) allowing the phases to settle for 5 to 90 minutes, (i) removing the aqueous phase from the reactor, (j) optionally repeating steps (g), (h), and (i) until the catalyst residue contents are less than 10 ppm, and (k) removing the polymer cement from the reactor and removing the solvent to recover the epoxidized polymer.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 10.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for the concurrent epoxidation of, and catalyst residue extraction from, anionically polymerized diene-containing polymers which have been hydrogenated using a Group VIII metal catalyst, said process comprising: (a) introducing a catalyst residue-containing diene-containing polymer cement into a reactor, (b) heating the polymer cement to a temperature of 25° to 65° C., (c) contacting the polymer cement with a caustic solution, (d) contacting the polymer cement with a peracid solution, (e) mixing the polymer, and acid at 25° to 65° C. for 1/2 to 3 hours, (f) optionally addin

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗