Abstract
A method for producing asphalt fibers includes supplying molten asphalt to a rotating asphalt spinner, centrifuging asphalt fibers from the asphalt spinner, and collecting the asphalt fibers. The molten asphalt is supplied to the asphalt spinner at a temperature within the range of from about 270° to about 500° F. Also disclosed is a method for integrating asphalt with reinforcement fibers including the steps of establishing a downwardly moving veil of reinforcement fibers, such as glass fibers, and centrifuging asphalt fibers from a rotating asphalt spinner positioned within the veil of reinforcement fibers to integrate the asphalt with the reinforcement fibers. A method for making an asphalt roofing shingle includes the steps of assembling together a mat of asphalt fibers with a mat of reinforcement fibers, coating the assembled mats to form an asphalt coated sheet, applying granules to the asphalt coated sheet, and cutting the asphalt coated sheet into roofing shingles. The invention also includes the asphalt roofing shingle made by this process. Further, the invention includes asphalt highway reinforcement products containing asphalt fibers, and the method of making such produc
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 23 · Forward citations: 15.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
Asphalt fibers having diameters less than about 250 Ht, the asphalt having a softening point within the range of from about 180° to about 350° F., where the asphalt has an asphaltene content within the range of 0 to 35 percent by weight of the asphalt material and is modified with one or more thermoplastic or thermoset organic modifiers, the modifiers being present in an amount within the range of from about 2 to about 30 percent by weight of the asphalt material.
- Claim 2Depends on #1
The asphalt fibers of claim 1 in which the asphalt is modified with one or more organic modifiers from the group consisting of natural rubber, synthetic rubber, elastomers, polymers, and resins.
- Claim 3Depends on #2
The asphalt fibers of claim 2 in which the modifiers are present in an amount within the range of from about 4 to about 12 percent by weight of the asphalt materia
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗