Patents
US 5,534,612 A#4245055 Most CitedExpiredUnited States (USPTO)Utility

Glass fiber binding compositions, process of making glass fiber binding compositions, process of binding glass fibers, and glass fiber compositions

20Forward Citations (#4245055 Global)
0.7/yrCitation Velocity (#11255172 Global)
3.21Citation PageRank (#6804315 Global)
50Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

The present invention relates to a glass fiber binding composition having an effective binding amount of an aqueous compatible furan resin mixed with sufficient water to result in a binding composition having from 0.5 to 80% nonvolatile. The aqueous compatible furan resin is the reaction product of a source of ammonia and a first reaction product, the first reaction product being derived from the reaction of an acidic furan resin, a source of reactable formaldehyde, and a formaldehyde scavenger. The invention further pertains to a process of binding glass fibers at junctions of the fibers comprising the steps of providing glass fibers, applying an effect binding amount of the binding composition of the invention to the glass fibers such that the binder is present at a portion of the junctions, and curing the resin at the junctions of the glass fibers. Finally, the invention also discloses glass fiber compositions comprising a plurality of glass fibers having a plurality of junctions where two or more fibers meet, and an effective binding amount of the binding composition of the invention.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 20.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method of making a glass fiber binding composition, comprising the steps of: providing an effective binding amount of an acidic furan resin; providing a source of reactable formaldehyde; mixing a formaldehyde scavenger with the furan resin in the presence of the source of reactable formaldehyde to form a first mixture; heating the first mixture to a temperature of less than 100 degrees C. for period of from 1 to 10 hours; adding a source of ammonia to the first mixture to form a second mixture; heating the second mixture to a temperature of less than 100 degree C. for a period of f

  2. Claim 2Depends on #1

    The method of claim 1 where the step of providing a furan resin comprises providing the reaction product resulting from the

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 20 total)

Non-Patent Literature (5)

  • A. Gandini, Polymers and Oligomers Containing Furan Rings, Agricultural and Synthetic Polymers, 1990, pp. 195 208. Developed from TX Symposium Apr. 9 14 1989.
  • A. Gandini, Polymers and Oligomers Containing Furan Rings, Agricultural and Synthetic Polymers, 1990, pp. 195-208. Developed from TX Symposium Apr. 9-14 1989.
  • C. R. Schmitt, Polyfurfuryl Alcohol Resins, Polymer Plast. Technol. Eng., 3(2), 1974, pp. 121 158.
  • C. R. Schmitt, Polyfurfuryl Alcohol Resins, Polymer-Plast. Technol. Eng., 3(2), 1974, pp. 121-158.
  • E. M. Wewerka et al., A Study of the Low Molecular Weight Components of Furfuryl Alcohol Polymers, J. of Applied Polymer Science, vol. 13, 1971, pp. 1437 1451.