US 5,516,548 A#43654119 Most CitedExpiredUnited States (USPTO)Utility

Tungsten disulfide modified bismaleimide

2Forward Citations (#43654119 Global)
0.1/yrCitation Velocity (#50618537 Global)
0.93Citation PageRank (#46287996 Global)
5Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A method of restoring a damaged surface of a metal substrate to a functional conditions through application of a filler material consisting essentially of bismaleimide and tungsten disulfide having a ratio of 10:1. The bismaleimide having been cured through the following sequence to maintain the durability thereof when exposed to aromatic fuels at temperatures up to 500° F., the temperature of the bismaleimide is uniformly raised from room temperature to 350° F. in one hour and maintained at 350° F. for an additional hour and thereafter the temperature is immediately raised to 475° F. and maintained at 475° F. for an additional two hours.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 2.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of restoring a damaged and/or worn surface on a metal substrate to substantially conform with an original surface profile, said method comprising the steps of: mixing a filler material consisting essentially of tungsten disulfide and bismaleimide together to obtain a uniform mixture; applying a quantity of filler material on said damaged and/or worn surface; placing said metal substrate in an oven; uniformly raising the temperature of said oven and said metal substrate to define a cure cycle for said bismaleimide, said cure cycle including: a one hour ramp from room temperature