Patents
US 5,503,733 A#9064931 Most CitedExpiredUnited States (USPTO)Utility

Process for phosphating galvanized steel surfaces

11Forward Citations (#9064931 Global)
0.4/yrCitation Velocity (#21674144 Global)
2.72Citation PageRank (#8848907 Global)
19Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

The invention relates to a process for phosphating galvanized steel surfaces, preferably electrolytically or hot-dip galvanized surfaces of steel strip, by treating them in a bath or spray with acidic aqueous phosphating solutions, wherein the workpieces are given a d.c. cathodic treatment at the same time. In the process, (a) the phosphating solutions contain Zn +2 cations in the range from 0.1 to 5 g/l, PO 4 -3 anions in the range from 5 to 50 g/l, NO 3 - anions in the range from 0.1 to 50 g/l, Mn +2 cations in the range from 0.1 to 5 g/l, and Cu +2 cations in the range from 0.001 to 1 g/l; (b) the following conditions are used: pH of the phosphating solution in the range from 1.5 to 4.5, temperature of the phosphating solution in the range from 10° to 80° C., treatment time in the range from 1 to 300 sec; and (c) the workpieces are also cathodically treated with a direct current with a density in the range from 0.01 to 100 mA/cm 2 during phosphating.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 19 · Forward citations: 11.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A process for phosphating galvanized steel surfaces by immersion or spray/immersion treatment thereof with acidic aqueous solutions wherein: a) the acidic aqueous solutions comprise: Zn 2+ cations in quantities of 0.1 to 5 g/l, PO 4 3- anions in quantities of 5 to 50 g/l, NO 3- anions in quantities of 0.1 to 50 g/l, Mn 2+ cations in quantities of 0.1 to 5 g/l and Cu 2+ cations in quantities of 0.001 to 1 g/l, b) the acidic aqueous solutions have a pH value of 1.5 to 4.5 and a temperature of 10° to 80° C. and are used for a treatment time of 1 to 300 seconds, and c) the g

  2. Claim 2Depends on #1

    A process as claimed in claim 1, wherein the acidic aqueous solutions comprise: Zn 2+ cations in quantities of 0.5

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (4)

  • "Die Phosphatierung von Metallen", Eugen G. Leuze Verlag, 2nd Edition 1988, pp. 20, 56, 79 et seq. and 107.
  • Die Phosphatierung von Metallen , Eugen G. Leuze Verlag, 2nd Edition 1988, pp. 20, 56, 79 et seq. and 107.
  • M. H. Abbas, Finishing, Oct. 1984, pp. 30 31.
  • M. H. Abbas, Finishing, Oct. 1984, pp. 30-31.