Patents
US 5,502,004 A#12391403 Most CitedExpiredUnited States (USPTO)Utility

Method for manufacturing a semiconductor device with heat treated diffusion layers

8Forward Citations (#12391403 Global)
0.3/yrCitation Velocity (#27261728 Global)
4.57Citation PageRank (#3832740 Global)
16Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

In a method for forming a metal wiring layer of a semiconductor device an insulating layer is formed on a semiconductor substrate having impurity-doped regions. A contact hole is formed in the insulating layer to expose an impurity-doped semiconductor region. Thereafter, a diffusion barrier layer is formed on the inner surface of the contact holes and on the surface of the semiconductor substrate exposed by the contact holes. The diffusion barrier layer is heat-treated for two minutes to one hour in a vacuum at a temperature of 450 DEG C. to 650 DEG C. Then, a metal wiring layer of a semiconductor device is formed on the diffusion barrier layer.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 16 · Forward citations: 8.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method for manufacturing a semiconductor device, comprising the steps of: forming an insulating layer on a semiconductor substrate having an impurity-doped region therein, the insulating layer having a contact hole exposing the impurity-doped region; forming a first diffusion barrier layer on the inner surface of the contact hole and on the surface of the semiconductor substrate which is exposed by the contact hole; after said step of forming the first diffusion barrier layer is completed, heat-treating the first diffusion barrier layer at a pressure no greater than about 4 mTorr; form

  2. Claim 2Depends on #1

    A method as in claim 1, wherein the first diffusion barri

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (16)

PatentTitleYearCitations
JP H01276743 AManufacture of semiconductor device—1
US 4,985,372 AMethod of forming conductive layer including removal of native oxide199186
US 5,010,032 AProcess for making CMOS device with both P+ and N+ gates including refractory metal silicide and nitride interconnects1991104
DD 291,877 A5Verfahren zum herstellen selbstjustierender silizidkontakte auf halbleiteranordnungen—1
JP H0467622 AManufacture of semiconductor device—4
US 5,094,981 ATechnique for manufacturing interconnections for a semiconductor device by annealing layers of titanium and a barrier material above 550° C.199259
EP 0,477,990 A2A method of enhancing the properties of a thin film on a substrate—22
JP H04214671 AMetallization method of rear of semiconductor substrate—6
US 5,236,868 AFormation of titanium nitride on semiconductor wafer by reaction of titanium with nitrogen-bearing gas in an integrated processing system1993123
US 5,240,880 ATi/TiN/Ti contact metallization199366
US 5,242,860 AMethod for the formation of tin barrier layer with preferential (111) crystallographic orientation199390
US 5,266,521 AMethod for forming a planarized composite metal layer in a semiconductor device199366
US 5,270,254 AIntegrated circuit metallization with zero contact enclosure requirements and method of making the same199351
US 5,278,099 AMethod for manufacturing a semiconductor device having wiring electrodes199449
US 5,300,455 AProcess for producing an electrically conductive diffusion barrier at the metal/silicon interface of a MOS transistor199430
US 5,395,795 AMethod for fabricating a semiconductor device199521