Process for producing carbon materials
Abstract
A process for producing an optically isotropic reformed pitch useful for various carbon materials is provided. This process comprises mixing a pitch having a ratio of aromatic hydrocarbon fa of more than 0.6 with a strong Lewis acid and a co-solvent so as to give a mol ratio of the said Lewis acid to the said pitch in the range of 0.3˜5.0 and a mol ratio of the said co-solvent to the said pitch in the range of ratio of 2.5˜50, reacting the mixture at a temperature of 100°˜300° C. and removing the Lewis acid and the co-solvent from the reaction product. Meso-Carbon microbeads having a uniform diameter of 20 μm or less can be produced at a high yield of 60% or more by heat treating the said reformed pitch at 200°˜380° C. to produce the optically anisotropic small spheres and separating them from an optically isotropic matrix.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 19 · Forward citations: 8.
Claims (2 — 2 Independent, 0 Dependent)
- Claim 1Independent Claim
A process for producing an optically isotropic reformed pitch useful for carbon materials which consists essentially of mixing a pitch having an aromatic carbon ratio fa of more than 0.6, with one Lewis acid selected from the group consisting of anhydrous AlCl 3 and HF.BF 3 and a co-solvent selected from the group consisting of dichlorobenzene, nitrobenzene and trichlorobenzene in an amount sufficient to dissolve both the said pitch and the said Lewis acid and promote a reaction in the liquid state, so as to give a mol ratio of the said Lewis acid to the said pitch in the range of 0.3-5.0 an
- Claim 2Independent Claim
A p
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗