Photodegradable cellulose ester tow
Abstract
The present invention is directed to a man-made fiber comprising a cellulose ester and 0.05 to 5.0% by weight of a titanium dioxide having an average particle size of less than 100 nanometers.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 28.
Claims (3 — 2 Independent, 1 Dependent)
- Claim 1Independent Claim
A man-made fiber comprising a mixture of: a cellulose ester; and about 0.05 to 5.0% by weight of titanium dioxide having an average particle size of less than 100 nanometers.
- Claim 2Independent Claim
A man-made fiber comprising a mixture of: a cellulose acetate having a degree of substitution of 1.5 to 2.7; about 0.05 to 5.0% by weight of titanium dioxide having an average particle size of less than 100 nanometers; and being adapted to be substantially degraded, as measured by AATCC TEST METHOD 169-1990, in 300 hours or less.
- Claim 3Depends on #2
The fiber according to claim 2 wherein said titanium dioxide in said cellulose acetate ranges from about 0.1 to 3.0% by weight.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 28 total)
References Cited — Backward Prior Art (6)
Non-Patent Literature (5)
- AATCC Test Method 177 1993, Colorfastness to Light at Elevated Temperature and Humidity: Water Cooled Xenon Lamp Appartus .
- AATCC Test Method 177-1993, "Colorfastness to Light at Elevated Temperature and Humidity: Water Cooled Xenon Lamp Appartus".
- AATCC Test Method 69 1990, Weather Resistance of Textiles: Xenon Lamp Exposure .
- AATCC Test Method 69-1990, "Weather Resistance of Textiles: Xenon Lamp Exposure".
- Brown, C. L. "The Design of Cigarettes", Hoechst Celanese Corporation, Charlotte, NC 1990 pp. 59-64.