Patents
US 5,489,342 A#18464473 Most CitedExpiredUnited States (USPTO)Utility

Method of manufacturing silicon steel sheet having grains precisely arranged in goss orientation

6Forward Citations (#18464473 Global)
0.2/yrCitation Velocity (#32765795 Global)
1.42Citation PageRank (#25021120 Global)
19Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

The present invention provides a method of manufacturing a silicon steel sheet having grains precisely arranged in the Goss orientation, comprising the steps of preparing a steel material containing 0.01 wt % or less of C, 2.5 to 7.0 wt % of Si, 0.01 wt % or less of S, 0.01 wt % or less of Al, 0.01 wt % or less of N, subjecting the steel material to hot rolling maintained 1000 DEG C. or higher such that the temperature of the rolled material at an end of the hot rolling step falls within the range of 700 DEG to 950 DEG C., subjecting the steel material to a primary cold rolling process at a rolling reduction of 30 to 85%, annealing the steel material at a temperature of 600 DEG to 900 DEG C., subjecting the steel material to a secondary cold rolling process at a rolling reduction of 40 to 80%, annealing the steel material again at a temperature of 600 DEG to 900 DEG C., subjecting the steel material to a tertiary cold rolling process at a rolling reduction of 50 to 75%, and annealing the steel material in a reducing atmosphere, or in a non-oxidizing atmosphere having an oxygen partial pressure of 0.5 Pa or less, or in a vacuum having an oxygen partial pressure of 0.5 Pa or less, at

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 19 · Forward citations: 6.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of manufacturing a silicon steel sheet having grains precisely arranged in a Goss orientation, comprising the steps of: (a) providing a steel material containing 0.01 wt % or less of C, 2.5 to 7.0 wt % of Si, 0.01 wt. % or less of S, 0.01 wt % or less of Al and 0.01 wt. % or less of N; (b) subjecting the steel material from step (a) which is maintained at a temperature of 1000° C. or higher to hot rolling such that the temperature of the resultant rolled material at the end of the hot rolling is 700° to 950° C.; (c) subjecting the steel material from step (b) to a primary cold rol

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (19)

PatentTitleYearCitations
US 3,089,795 AMethod for producing fiber texture and cube-texture sheets of iron-base alloys196312
US 3,152,929 AProcess for producing silicon steel with preferred orientation19643
US 3,586,545 AMethod of making thin-gauge oriented electrical steel sheet19714
DE 2,316,808 A1Verfahren zum herstellen eines kornorientierten elektroblechs mit hoher magnetischer flussdichte—5
US 3,841,924 AMethod for producing a high magnetic flux density grain oriented electrical steel sheet197415
US 3,932,234 AMethod for manufacturing single-oriented electrical steel sheets comprising antimony and having a high magnetic induction197653
US 4,251,295 AMethod of preparing an oriented low alloy iron from an ingot alloy having a high initial sulfur content19814
GB 2,101,631 AProducing a grain-oriented electromagnetic steel sheet having a high magnetic flux density by controlled precipitation annealing—7
US 4,439,252 AMethod of producing grain-oriented silicon steel sheets having excellent magnetic properties19846
US 4,469,533 AMethod of producing grain oriented silicon steel sheets or strips having high magnetic induction and low iron loss19849
US 4,473,416 AProcess for producing aluminum-bearing grain-oriented silicon steel strip198421
EP 0,047,129 B1Grain-oriented silicon steel sheets having a very low iron loss and methods for producing the same198524
JP S6267115 AProduction of light-gage grain oriented electrical steel sheet of low iron loss—2
EP 0,229,846 A1Process for producing silicon steel sheet having soft magnetic characteristics—8
EP 0,234,443 A2Process for producing a grain-oriented electrical steel sheet having improved magnetic properties—10
JP S6455339 AProduction of grain-oriented silicon iron alloy thin band—7
JP H0257635 AManufacture of extra thin foil of grain-oriented silicon steel with low core loss—6
EP 0,390,142 A2Process for producing grain-oriented electrical steel sheet having high magnetic flux density—15

Non-Patent Literature (2)

  • Patent Abstracts of Japan, vol. 14, No. 232 (C 719) (4175), May 17, 1990; & JP A 02 057635 (Babcock Hitachi) Feb. 27, 1990.
  • Patent Abstracts of Japan, vol. 14, No. 232 (C-719) (4175), May 17, 1990; & JP-A-257635 (Babcock Hitachi) Feb. 27, 1990.