US 5,487,945 A#11447427 Most CitedExpiredUnited States (USPTO)Utility

Diamond films on nondiamond substrates

9Forward Citations (#11447427 Global)
0.3/yrCitation Velocity (#25465355 Global)
2.29Citation PageRank (#11703898 Global)
11Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A method for making an oriented diamond film includes the steps of seeding a face of a nondiamond substrate with diamond particles, and orienting the diamond particles with respect to the substrate by heating the seeded substrate to a predetermined temperature and for a predetermined time to dissolve portions of the diamond particles into the substrate while suppressing graphite formation. Diamond may then be deposited onto the oriented diamond particles by CVD techniques to thereby form an oriented diamond film on the nondiamond substrate. The nondiamond substrate is preferably a single crystal transition metal capable of dissolving carbon. The transition metal is preferably selected from the group consisting of nickel, cobalt, chromium, magnesium, iron, and alloys thereof. For nickel as the substrate material, the temperature for orientation of the diamond particles is preferably about 1200° C., for a time period in the range of about 1 to 15 minutes, and, more preferably, about 1 to 5 minutes. Structures produced by the method are also disclosed and include the absence of a graphite layer between the diamond and the nondiamond substrate.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 9.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A structure comprising: a nondiamond substrate having a face and comprising a transition metal capable of dissolving carbon; and a plurality of oriented diamond seeds partially dissolved into the face of said substrate and being oriented so that individual diamond seeds are in alignment with a lattice of corresponding adjacent portions of said substrate.

  2. Claim 2Depends on #1

    A structure according to claim 1 wherein said diamond seeds are partially dissolved into the face of said substrate without an intervening layer of graphite.

  3. Claim 3Depends on #1

    A structure according to claim 1 further comprising a layer of diamond on said plurality of oriented diamond seeds.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • Bovenkerk et al., "Preparation of Diamond", Nature, pp. 1094-1098, Oct. 10, 1959.
  • Bovenkerk et al., Preparation of Diamond , Nature, pp. 1094 1098, Oct. 10, 1959.
  • D. S. Olson et al., "Growth of Diamond From Sputtered Atomic Carbon and Atomic Hydrogen", Mat. Res. Soc. Symp. Proc. vol. 270.
  • D. S. Olson et al., Growth of Diamond From Sputtered Atomic Carbon and Atomic Hydrogen , Mat. Res. Soc. Symp. Proc. vol. 270.
  • E. Hartmann, "On the Orientation Effects of Capillary Forces", Acta Physica Academiae Scientiarum Hungaricae, Tomus 47 (1-3), pp. 185-188 (1979).