Silica supported transition metal catalyst
Abstract
A transition metal containing catalyst useful for the polymerization of α-olefins is prepared by (A) forming in an inert atmosphere which excludes oxygen and moisture a slurry of (1) a porous inorganic oxide support material selected from the group consisting of silica, alumina, or a combination of silica and alumina, said support material containing not greater than about 5 millimoles of hydroxyl groups per gram of support material and a particle size not greater than about 10 microns and a surface area of from about 50 to about 800 m 2 /g in an inert organic liquid medium; (B) mixing said slurry with (2) an alkoxide and stirring the resultant mixture at a temperature of from about -20° C. to about 120° C. for a time sufficient to saturate the surface of the support material; (C) mixing the product form (B) with (3) a titanium compound or a combination of a titanium compound and (4) a vanadium compound and stirring the resultant mixture at a temperature of from about -20° C. to about 120° C. for a time sufficient to allow complete reaction of the titanium compound and the vanadium compound with the organomagnesium moieties remaining on the solid support; (D) mixing the product fro
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 22 · Forward citations: 24.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
In a process for extruding an ethylene/alpha-olefin copolymer into a film, the improvement comprising employing as said ethylene/alpha-olefin copolymer one having greater than about 17 percent high density fraction and a M w /M n ratio of less than about 3.6 to form a film having a gauge from about 0.4 to about 1.2 mils, a percent ultimate stretchability of at least about 280, and a puncture resistance of at least about 250 ft-lbs/cm 3 .
- Claim 2Depends on #1
The process of claim 1 wherein the ethylene/alpha-olefin copolymer has a density from about 0.905 g/cm 3 to about 0.935 g/cm 3 and a melt index from about 0.6 g/10 minutes to about 6 g/10 minutes.
- Claim 3Depends on #2
The process of claim 2 wherein the ethylene/alpha-olefin copolymer has a Mw/Mn ratio less than about 3.3 and a percent high density fraction of at least about 20.