Heat-resistant, propylene resin-based molding materials and molded products obtained therefrom
Abstract
There is provided a heat-resistant, propylene resin-based molding material, comprising the following components (A) and (B): component (A): 3 to 97% by weight of a resin-impregnated glass fiber bundle comprising: constituent (a1): 20 to 80 parts by weight of glass fibers having a length of at least 3 mm and an average diameter of 20 mu m or less, and constituent (a2): 80 to 20 parts by weight of a crystalline propylene polymer at least partly modified with an unsaturated carboxylic acid or a derivative thereof, the MFR of the modified polymer being 50 g/10 min or more, in which the glass fibers are present in the constituent (a2) in such a state that they are arranged almost in parallel with one another; and component (B): 97 to 3% by weight of a crystalline propylene polymer having an MFR of 50 g/10 min or more.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 13 · Forward citations: 19.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A heat resistant, propylene resin-based molding material, comprising the following components (A) and (B): component (A): 3 to 97% by weight of a resin-impregnated glass fiber bundle comprising: constituent (a 1 ): 20 to 80 parts by weight of glass fibers having a length of at least 3 mm and an average diameter of 20 μm or less, and constituent (a 2 ): 80 to 20 parts by weight of a crystalline propylene polymer at least partly modified with an unsaturated carboxylic acid or a derivative thereof, the MFR of the modified polymer being 50 g/10 min or more, said resin-impregnated glass fiber
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗