Patents
US 5,484,748 A#15288700 Most CitedExpiredUnited States (USPTO)Utility

Method for storage of silicon wafer

7Forward Citations (#15288700 Global)
0.2/yrCitation Velocity (#30742488 Global)
1.75Citation PageRank (#18037152 Global)
5Prior Art Cited
3Claims (2 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

The single crystal silicon wafers which have undergone a treatment with a chemical liquid such as an acid or an alkali are stored without entailing contamination of their surfaces by causing the wafers to be immediately immersed, either directly or after being washed with water, in an aqueous hydrogen peroxide solution. The prevention of the contamination of surfaces of the wafers is attained effectively by setting the concentration of hydrogen peroxide in the aqueous hydrogen peroxide solution in the range of from 0.01 to 30% by weight and the temperature of the aqueous hydrogen peroxide solution at the time that the wafers are immersed in the solution in the range of from 10° to 30° C.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 7.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method for the storage of silicon wafers, which is characterized by causing silicon wafers which have undergone a treatment with such a chemical liquid as an acid or an alkali solution to be immediately immersed, either directly or after being washed with water, in an aqueous hydrogen peroxide solution, and storing said silicon wafers therein until the next component process.

  2. Claim 2Depends on #1

    A method according to claim 1, wherein the concentration of hydrogen peroxide in said aqueous hydrogen peroxide solution is in the range of from 0.01 to 30% by weight, preferably from 0.05 to 1% by weight, and the temperature of said aqueous hydrogen peroxide solution at the time that single crystal silicon wafers are immersed therein is in the range of from 0° C. to 80° C., preferably from 10° C. to 30° C.

  3. Claim 3Independent Claim

    A method according to cla

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • C. Okada, et al., Jpn. J. Appl. Phys., 32 (1993) L1031 "Accumulation of Organic Matter on Bare Si Wafer in Air".
  • C. Okada, et al., Jpn. J. Appl. Phys., 32 (1993) L1031 Accumulation of Organic Matter on Bare Si Wafer in Air .
  • M. Grunder, J. Vac. Sci. Technol., A5, 4 (1987) 2011 HREELS Measurements on Hydrophilic Si (100) Wafers . . . .
  • S. Wolf & R. N. Tauber, "Silicon Processing for the VLSI Era", 1986 vol. I, pp. 514-521, 531-535.
  • S. Wolf & R. N. Tauber, Silicon Processing for the VLSI Era , 1986 vol. I, pp. 514 521, 531 535.