Thermoplastically processible elastomers with improved optical properties
Abstract
Thermoplastically processible elastomers based on acrylates, which contain 40-100 wt. % of one or more comb polymers having a molecular weight greater than 50,000 Dalton, comprised of: (A) 5-50 wt. % of macromonomers comprised of methyl methacrylate or copolymers of methyl methacrylate with comonomers chosen from other (meth)acrylic acid esters and styrenes; containing a terminal unit with a radically polymerizable group and having a glass transition temperature (Tg) of at least 60° C., a molecular weight in the range 500-100,000 Dalton, and an index of refraction in the range n D =1.48-1.50; (B) 5-90 wt. %, based on the total weight of the comb polymer, of monomers or monomer mixtures of formula I: ##STR1## where R 1 is a C 1 -C 12 -alkyl group; and (C) 5-50 wt. % based on the total weight of the comb polymer, of a phenyl group-containing radically polymerizable monomer.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 8.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A thermoplastically processible elastomer composition comprising 40-100 wt. % of a comb polymer of improved optical properties, said polymer having a molecular weight greater than 50,000 Daltons, said comb polymer comprising a main chain having macromonomer side chains pendant therefrom, said macromonomer containing a terminal unit with a radically polymerizable group, said group constituting a monomer unit of said main chain, said comb polymer main chain comprising: (A) 5-50 wt. % of a hydrophobic macromonomer consisting essentially of polymerized methyl methacrylate or a polymerized copolyme
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗