Patents
US 5,456,943 A#9405659 Most CitedExpiredUnited States (USPTO)Utility

Method for the preparation of electrically conductive infrared-reflecting layers on glass, glass-ceramic or enamel surfaces

11Forward Citations (#9405659 Global)
0.3/yrCitation Velocity (#22336760 Global)
2.12Citation PageRank (#13278313 Global)
7Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A method is described for the preparation of electrically conductive, infrared-reflecting layers on glass, glass-ceramic or enamel surfaces by spraying and thermally decomposing liquid Sn(IV) compounds and fluorine compounds as preparations containing doping agents on to the surface heated to 400° to 800° C., yet below their softening point, wherein, as liquid preparations, ionically stabilized, organic tin(IV) acid sols are used, which contain aliphatic alcohols or ketones with, in each case, at most 6 carbon atoms in the molecule or esters with a boiling point below 180° C. as liquid, organic medium, as well as fluoride ions in an adequate amount for doping. The preparations are homogenous, stable for a long time, and can readily be diluted with alcohols, ketones, and other polar solvents. The tin oxide layers, produce with the preparations on the substrates, have a high transparency in the wavelength of visible light, a low surface resistance and a high reflection in the infrared wavelength region.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 11.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method of preparing an electrically, conductive, infrared-reflecting layer on a glass, glass-ceramic or enamel surface having a softening point, comprising: forming a liquid organic tin (IV) acid sol composition, and doping said liquid organic tin (IV) acid sol composition with a fluorine containing compound, heating said surface to 400° C. to 800° C. below its softening point, and spraying and decomposing said composition unto said substrate, wherein said liquid organic tin (IV) acid sol composition comprises aliphatic alcohols or ketones both having, at most, 6 carbon atoms in a mole

  2. Claim 2Depends on #1

    The method of claim 1, wherein the tin (IV) acid sol is obtained by the reaction of a compound selected from the group consisting of tin (II) chloride, tin (II) oxalate and tin (II) acetate with hyd

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (2)

  • Yi, "Sol-Gel Processing of Complex Oxide Films" Ceramic Bulletin vol. 70 No. 7 1991 pp. 1173-1179.
  • Yi, Sol Gel Processing of Complex Oxide Films Ceramic Bulletin vol. 70 No. 7 1991 pp. 1173 1179.