Pulp-like short fibers from liquid crystal polyesters
Abstract
Pulp-like short fibers prepared from liquid crystal polyesters capable of forming an anisotropic melt phase at a temperature of 200 DEG C. to 400 DEG C. and having a molecular weight of 2,000 to 100,000 are provided. These fibers consist of microfibrils and have the following highly-oriented fiber characteristics and properties: (a) Tensile strength: 5-30 g/den.; (b) Modulus of elasticity: 200-1,500 g/den.; (c) Orientation angle as determined by an X-ray diffraction: below 20 DEG ; (d) Thickness distribution: 0.1-50 mu m; (e) Length distribution: 0.1-50 mm; and (f) Specific surface area as determined by a nitrogen adsorption method: 3-30 m2/g.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 21 · Forward citations: 9.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
Pulp-like short fibers prepared by first heating liquid-crystalline polyesters capable of forming an anisotropic melt phase at a temperature of 200° C. to 400° C. and having a molecular weight of 2,000 to 100,000 at a temperature sufficient to melt them completely to give a uniform hot melt, and then cooling the hot melt to a temperature just above its melting point to form an anisotropic melt, followed by extrusion, said fibers having a good dispersibility and easiness in manufacturing paper, and the following highly-oriented fiber characteristics and properties: (a) Tensile strength: 5-30 g/
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗