Patents
US 5,454,887 A#2519829 Most CitedExpiredUnited States (USPTO)Utility

Process for manufacturing a medium-carbon steel plate with improved formability and weldability

28Forward Citations (#2519829 Global)
0.9/yrCitation Velocity (#7910225 Global)
4.92Citation PageRank (#3397868 Global)
8Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A process for manufacturing a medium-carbon steel plate having a graphitization of 50% or more with improved formability and weldability is disclosed, the process comprises the steps of: hot rolling a steel with a finishing temperature of 700 DEG -900 DEG C., the alloy composition of the steel consisting essentially of, by weight %: C: 0.20-0.70%, Si: more than 0.20 but not more than 2.00%, Mn: 0.05-0.50%, P: not more than 0.020%, S: not more than 0.010%, sol. Al: 0.01-1.00%, B: 0.0003-0.0050%, N: 0.002-0.010%, B/N: 0.2-0.8, Cu: 0-1.00%, Ni: 0-2.00%, Ca: 0-0.010%, and Fe and incidental impurities: balance, cooling the resulting hot-rolled steel plate at a cooling rate of 5 DEG -50 DEG C./s, coiling the steel plate at a temperature of 400 DEG -650 DEG C., and optionally, cold rolling the hot-rolled steel plate with a reduction in thickness of 20-85%, and annealing the cold-rolled steel plate at a temperature of 600 DEG - Ac1 for 1 hour or longer.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 28.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for manufacturing a medium-carbon steel plate having a graphitization of 50% or more with improved formability and weldability, which comprises the steps of: hot rolling a steel with a finishing temperature of 700°-900° C., the steel consisting essentially of, by weight %: C: 0.20-0.70%, Si: more than 0.20 but not more than 2.00%, Mn: 0.05-0.50%, P: not more than 0.020%, S: not more than 0.010%, sol. Al: 0.01-1.00%, B: 0.0003-0.0050%, N: 0.002-0.010%, B/N: 0.2-0.8, Cu: 0-1.00%, Ni: 0-2.00%, Ca: 0-0.010%, and Fe and incidental impurities: balance, cooling the resulting

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 28 total)

PatentTitleYearCitations
US 2005258145 A1Weldment of different materials and resistance spot welding method—1
CN 119,776,623 AManufacturing method for improving uneven hardness of cold-rolled medium-high carbon strip steel in width direction after heating in bell-type annealing furnace—0
US 2008289726 A1Cold rolled, dual phase, steel sheet and method of manufacturing same—4
US 10,077,491 B2High carbon hot rolled steel sheet and method for manufacturing the same20180
US 9,157,138 B2Complex metallographic structured high strength steel and method of manufacturing20153
US 2006108035 A1Cold rolled, dual phase, steel sheet and method of manufacturing same—37
US 8,366,844 B2Method of making hot rolled dual phase steel sheet20137
US 11,155,902 B2High strength, hot dip coated, dual phase, steel sheet and method of manufacturing same20210
US 2010043925 A1High strength, hot dip coated, dual phase, steel sheet and method of manufacturing same—11
US 5,648,044 AGraphite steel for machine structural use exhibiting excellent free cutting characteristic, cold forging characteristic and post-hardening/tempering fatigue resistance199710
US 6,673,171 B2Medium carbon steel sheet and strip having enhanced uniform elongation and method for production thereof200423
US 7,473,864 B2Weldment of different materials and resistance spot welding method20096
US 7,879,160 B2Cold rolled dual-phase steel sheet201111
US 7,959,747 B2Method of making cold rolled dual phase steel sheet20116
EP 2,733,228 A4Hot press forming steel plate, formed member using same, and method for manufacturing the plate and member—0