Defect-free bipolar process

13Forward Citations (#7310267 Global)
0.4/yrCitation Velocity (#19167518 Global)
3.63Citation PageRank (#5575477 Global)
10Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A method for manufacturing bipolar semiconductor devices wherein damage to the active regions of the devices due to the direct implantation of impurities is suppressed. A material is selectively deposited on a semiconductor substrate, the material having a characteristic such that formation of the material occurs on some substances such as silicon and polysilicon, and formation of the material is suppressed on other substances such as silicon dioxide and silicon nitride. Impurities are introduced into the material rather than into the substrate. The impurities are then diffused into the active regions by standard processes such as rapid thermal anneal (RTA) or furnace anneal. The material generally contains germanium, and usually is a polycrystalline silicon-germanium alloy. The diffusion depth of the impurities may be controlled with great precision by manipulating several parameters. The parameters include the thickness of the material, the energy of the impurity implants, the density of the impurity implants, and the concentration of germanium in the material.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 13.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method for manufacturing a bipolar device wherein damage to active regions of the device due to direct implantation of impurities is suppressed, the bipolar device having an oxide layer in which apertures have been formed for base, emitter, and collector contacts, the method comprising the steps of: selectively depositing a buffer material on the active regions in the apertures in the oxide layer, the buffer material comprising germanium; implanting a first impurity of a first conductivity type into the buffer material formed in the base contact aperture; implanting a second impurity of

  2. Claim 2Depends on #1

    The method of claim 1 wherein the buffer material comprises a

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • Aronowitz, S. "Dopant diffusion control in silicon using germanium," J. Appl. Phys. 68(7), 1 Oct. 1990, pp. 3293-3297.
  • Aronowitz, S. Dopant diffusion control in silicon using germanium, J. Appl. Phys. 68(7), 1 Oct. 1990, pp. 3293 3297.
  • Aronowitz, S. et al. "Damage Freeze-in Phenomena as a Function of Dopant Implant; Type in Germanium-Rich Regions in Silicon," Mat. Res. Soc. Symp. Proc., vol. 209, 1991, pp. 481-487.
  • Aronowitz, S. et al. Damage Freeze in Phenomena as a Function of Dopant Implant; Type in Germanium Rich Regions in Silicon, Mat. Res. Soc. Symp. Proc., vol. 209, 1991, pp. 481 487.
  • Coffa, S. et al. "Arsenic influence on extended defects produced in silicon by ion implantation," Appl. Phys. Lett. 56(24) 11 Jun. 1990, pp. 2405-2407.