Air electrode bodies for solid oxide fuel cells, a process for the production thereof, and a production of solid oxide fuel cells
Abstract
An air electrode body for a solid oxide fuel cell, which is composed of a perovskite-type structure having a chemical composition of (La1-xAx)1-yMnO3 wherein 0<x</=0.5, 0<y</=0.2, and A is at least one metal selected from strontium, calcium, manganese, barium, yttrium, cerium and ytterbium. The air electrode body has a porosity of 15 to 40% and an average pore diameter of 1-5 mu m. A process for producing the air electrode body, includes the steps of: mixing lanthanum or a lanthanum compound, manganese or a manganese compound, a metal A or a compound of the metal A wherein A is at least one kind of metals selected from the group of strontium, calcium, manganese, barium, yttrium, cerium and ytterbium; calcining the resulting mixture at a temperature from 1,300 DEG C. to 1600 DEG C. to synthesize (La1-xAx)1-yMnO3; grinding the synthesized material to a powder having an average particle diameter of 3 to 15 mu m; adding at least an organic binder, water and 2 to 12 parts by weight of a pore-forming agent to 100 parts by weight of the resulting powder and kneading the resulting mixture; molding the kneaded material; drying the molding; and then firing the molding at a temper
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 13 · Forward citations: 54.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
An air electrode body for a solid oxide fuel cell, said air electrode body being constituted by a perovskite structure having a chemical composition of (La 1-x A x ) 1-y MnO 3 , wherein 0<x≦0.5, 0<y≦0.2, and A is at least one metal selected from the group consisting of strontium, calcium, magnesium, barium, yttrium, cerium and ytterbium, said air electrode body having a porosity of 15 to 40% and an average pore diameter of 1-5 μm.
- Claim 2Depends on #1
The air electrode body as set forth in claim 1, wherein the porosity and the average pore diameter of the air electrode body are 25-35% and 1-3 μm, respectively.
- Claim 3Depends on #1
The air electrode body as set forth in claim 1, wherein 0.1≦x≦0.3 and 0<y≦0.1.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 54 total)
References Cited — Backward Prior Art (13)
Non-Patent Literature (5)
- "A comprehensive engineering for energies", 13-2, 1990, pp. 52-68.
- "Stability of Perovskite Oxide Electrode with Stabilized Zirconia", Yamamoto et al., Dept. of Chemistry, Faculty of Engineering, Mie University, 1989, pp.87-92.
- A comprehensive engineering for energies , 13 2, 1990, pp. 52 68.
- Comm. Eur. Communities; Solid Oxide Fuel Cells 2 5 Jul. 1991, Greece EUR 13564, pp. 673 680, H. Kaneko et al., Reaction of La1 xCaxMnO3 Cathode with YSZ and its Influence on the Electrode Characteristics .
- Comm. Eur. Communities; Solid Oxide Fuel Cells 2-5 Jul. 1991, Greece--EUR 13564, pp. 673-680, H. Kaneko et al., "Reaction of La1-xCaxMnO3 Cathode with YSZ and its Influence on the Electrode Characteristics".