Patents
US 5,451,333 A#6681911 Most CitedExpiredUnited States (USPTO)Utility

Haze resistant dispersant-detergent compositions

14Forward Citations (#6681911 Global)
0.5/yrCitation Velocity (#17877356 Global)
3.64Citation PageRank (#5534974 Global)
50Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

According to the present invention, oleaginous compositions having improved stability are provided, wherein high molecular weight ashless dispersants and metal detergents are pre-blended at a temperature of at least 100° C. for a period of from 1 to 10 hours, cooled to at least 85° C. and admixed with additional additives, including oil soluble copper antioxidants and zinc dialkyl dithiophosphate antiwear agents.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 14.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A haze resistant composition comprising a reaction product prepared by (i) contacting a mixture comprising a major proportion of an oil of lubricating viscosity, from 3 to 45 weight percent on an active ingredient basis ashless dispersant and from 3 to 45 weight percent on an active ingredient basis metal detergent at a temperature of at least about 100° C. to form a heat treated mixture; (ii) cooling said heat treated mixture to a temperature of not greater than about 85° C. to form a cooled mixture; and (iii) thereafter adding a minor amount of at least one member selected from the group

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (2)

  • Research Disclosure, Oct. 1985, "Heat Treatment of Lubricant Additives", Disclosed anonymously, p. 25804.
  • Research Disclosure, Oct. 1985, Heat Treatment of Lubricant Additives , Disclosed anonymously, p. 25804.