Solid state polymerization process for foamed poly(ethylene naphthalate)
Abstract
This invention includes a process for preparing a solid state polymerized poly(ethylene naphthalate)or PEN polymer comprising: (1) preparing a molten PEN polymer with an intrinsic viscosity of from about 0.25 dl/g to about 0.55 dl/g, (2) dispersing an inert gas into the molten PEN polymer to form a foamed PEN polymer with a void fraction of from about 0.10 to about 0.50, (3) forming the foamed PEN polymer into granules, (4) devolatilizing the granular PEN polymer at a temperature of from about 80° C. to about 140° C., (5) crystallizing the devolatilized PEN polymer at a temperature of from about 150° C. to about 260° C., and (6) solid state polymerizing the crystallized PEN polymer at a temperature of from about 235° C. to about 265° C. to form a solid state polymerized PEN product.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 9 · Forward citations: 15.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A process for making a high molecular weight solid state polymerized poly(ethylene naphthalate) polymer comprising: preparing a molten poly(ethylene naphthalate) polymer with an intrinsic viscosity of from about 0.25 dl/g to about 0.55 dl/g; dispersing an inert gas into the molten poly(ethylene naphthalate) polymer to form a foamed poly(ethylene naphthalate) polymer with a void fraction of from about 0.10 to about 0.50; forming the foamed poly(ethylene naphthalate) polymer into granules suitable for solid state polymerization; devolatilizing the granular poly(ethylene naphthalate) polyme
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗