Method of manufacturing an ITO sintered body
Abstract
The invention encompasses a method for manufacturing a high density indium oxide/tin oxide (ITO) sintered body, as well as the ITO sintered body itself. The method produces an ITO sintered body of high homogeneity for use as a sputtering target in manufacturing processes where thin, transparent and electrically conductive ITO layers are deposited over transparent substrates. The method comprises the steps of preparing a slurry whose solid constituents consist of a finely divided mixture of between 99 and 50 weight percent of In 2 O 3 and 1 to 50 weight percent of SnO 2 , and between about 0.05 through 0.25 percent of a sintering agent formed from an oxide of, only one of the group consisting of aluminum, magnesium, yttrium, and silicon; forming the resulting slurry into a green body having a density of between about 4.0 and 4.8 gm/c 3 and heating the green body to a sintering temperature of between about 1500 and 1600 C. while maintaining a flow of oxygen over the green body sufficient to avoid the creation of a reducing atmosphere around the body, but insufficient to cause substantial disassociation of the In 2 O 3 and SnO 2 . The green body may be formed by casting the resulting
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 47.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method for manufacturing a high density ITO sintered body of high homogeneity, comprising: preparing a slurry whose solid constituents consist of a finely divided mixture of In 2 O 3 , SnO 2 and between about 0.05 and 0.25 percent by weight of a sintering agent consisting of only one oxide selected from the group consisting of aluminum oxide, calcium oxide, yttrium oxide, cesium oxide, magnesium oxide and silicon dioxide; forming said slurry into a green body having a density of between about 4.2-4.8 gm/c 3 , and heating said green body to a sintering temperature in an oxygen atmospher
- Claim 2Depends on #1
The method of claim 1, wherein said green body is heated for a time period of between 4 and 20 hours.
- Claim 3Depends on #1
The method of claim 1, wherein said oxide is SiO 2 .
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 47 total)
References Cited — Backward Prior Art (8)
Non-Patent Literature (2)
- Reed, James S., Introduction to the Principles of Ceramic Processing, John Wiley & Sons, New York, 1988, pp. 440 445.
- Reed, James S., Introduction to the Principles of Ceramic Processing, John Wiley & Sons, New York, 1988, pp. 440-445.