Abstract
A glass fiber forming composition exhibits a remarkably high dielectric constant epsilon GAMMA as well as superior chemical resistance, yet it is readily spun into glass fibers. The composition is characterized to show a devitrification temperature which is lower than a spinning temperature at which the glass composition exhibits a viscosity of 102.5 poise, so as to be readily spun into corresponding glass fibers. The composition consists essentially of 40 to 65 mol % of SiO2; 20 to 45 mol % of at least one component selected from the group consisting of MgO, CaO, SrO and BaO; 5 to 25 mol % of at least one component selected from the group consisting of TiO2 and ZrO2; and 0.5 to 15 mol % of NbO5/2 as calculated from an incorporated amount of Nb2O5. Alternately, the composition consist essentially of 40 to 65 mol % of SiO2; 20 to 45 mol % of at least one component selected from the group consisting of CaO, SrO and BaO; 5 to 25 mol % of at least one component selected from the group consisting of TiO2 and ZrO2; 0.5 to 15 mol % of NbO5/2 as calculated from an incorporated amount of Nb2O5; and 0.5 to 15 mol % of AlO3/2 as calculated from an incorporated amount of Al2O3. The composition
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 12 · Forward citations: 20.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A glass fiber forming composition consisting essentially of 0 to 15 mol % of at least one oxide selected from the group consisting of TaO 2 .5, LaO 1 .5, CeO 2 , ZnO, Li 2 O, Na 2 O, K 2 O, MnO 2 , and BO 1 .5, and 85-100 mol % of an oxide mixture, said oxide mixture consisting essentially of: 40 to 65 mol % of SiO 2 ; CaO, SrO and BaO each being present, said CaO, SrO and BaO being present in respective amounts which total 20 to 45 mol % of the oxide mixture; TiO 2 and ZrO 2 in amounts which total 5 to 25 mol % of the oxide mixture; and 0. 5 to 15 mol % of NbO 5/2 ; said compositio
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 20 total)
References Cited — Backward Prior Art (12)
Non-Patent Literature (4)
- Patent Abstracts of Japan, vol. 13, No. 461 (C 645) 18 Oct. 1989 & JP A 01 179 741, Jul. 17, 1989.
- Patent Abstracts of Japan, vol. 13, No. 461 (C-645) 18 Oct. 1989 & JP-A-01 179 741, Jul. 17, 1989.
- World Patents Index Latest, Week 03, Derwent Publications Ltd., AN 90 096954 & JP A 2 050 834, Feb. 20, 1990.
- World Patents Index Latest, Week 03, Derwent Publications Ltd., AN 90-096954 & JP-A-2 050 834, Feb. 20, 1990.