Patents
US 5,407,600 A#2909592 Most CitedExpiredUnited States (USPTO)Utility

Stable aqueous alumina sol and method for preparing the same

26Forward Citations (#2909592 Global)
0.8/yrCitation Velocity (#8646134 Global)
2.71Citation PageRank (#8947317 Global)
8Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A stable aqueous sol of amorphous alumina containing Al 2 O 3 up to 15% by weight and 0.1 to 0.5 gram equivalent of an anion of acid to 1 mol of aluminum in the sol, in which the colloidal particles of amorphous alumina have a controlled thickness in a range of 20 to 100 millimicrons and a uniform length in a range of 200 to 500 millimicrons is produced by a process comprising feeding an aqueous solution of an acid into an aqueous slurry containing 1 to 7% by weight of metallic aluminum, 10 to 200 ppm by weight as Si0 2 of a water-soluble silicate and 0 to 20 ppm by weight of a water-soluble sulfate as S0 4 to the water in the slurry while maintaining the slurry at a temperature of 80° C. to boiling point under normal pressure, said acid being in an amount of 0.1 to 0.5 gram equivalent to 1 mol of the metallic aluminum in said slurry, at a rate of 0.001 to 0.03 gram equivalent of the acid to 1,000 g of the water in the slurry per minute, and continuing heating the slurry after completion of the feeding of the acid at a temperature of 80° C. to boiling point of the slurry until a sol of amorphous alumina having a uniform length of 200 to 500 millimicrons is formed.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 26.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for preparing a stable aqueous sol of amorphous alumina containing Al 2 O 3 in an amount up to 15% by weight and an anion of acid in an amount of 0.1 to 0.5 gram equivalent to 1 mol of aluminum in the sol, in which the colloidal particles of amorphous alumina have a uniform thickness in a range of 40 to 100 millimicrons and a uniform length in a range of 200 to 500 millimicrons, the length being 5 to 10 times the thickness, comprising feeding an acid into an aqueous slurry of metallic aluminum while maintaining the slurry at a temperature of 80° C. to boiling point under normal pres

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗