Process for obtaining polyamide yarns with better output efficiency
Abstract
An improved output efficient polyamide-based preoriented yarn spun at a speed of at least 4000 m/min and obtained by introducing, before the spinning, of a quantity of 0.05 to 1% by weight of pyrogenic silica of particle size of between 5 and 15 nm into the molten polymer in the form of dispersion in a master mix of the same polyamide as that intended to be processed, the filaments after spinning being then cooled by means of a gas stream at room temperature and then sized and wound at a speed of between 4200 and 5800 m/min. The preoriented yarns thus prepared exhibit a delay in the orientation and are obtained with a gain in output efficiency of at least 10%, generally at least 15%.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 22 · Forward citations: 1.
Claims (2 — 2 Independent, 0 Dependent)
- Claim 1Independent Claim
Undrawn preoriented polyamide yarns containing from 0.05 to 1% by weight of uniformly distributed pyrogenic silica of particle size of between 5 and 15 nm, said yarns exhibiting a delay in orientation.
- Claim 2Independent Claim
Undrawn preoriented polyamide yarns containing from 0.5 to 1% by weight of pyrogenic silica of particle size of between 5 and 15 nm, said yarns exhibiting a delay in orientation, said yarn being obtained by introducing a quantity of 0.05 to 1% by weight of pyrogenic silica of particle size of between 5 and 15 nm into molten polyamide polymer in the form of a dispersion in a master mix of said same polyamide, spinning said polymer at a speed of at least 4000 m/min into filaments, cooling said filaments by means of a gas stream at room temperature and then sizing and winding said filaments at a
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (1 of 1 total)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 5,514,471 A | High-strength polyamide fiber | 1996 | 5 |
References Cited — Backward Prior Art (22)
Non-Patent Literature (2)
- World Patent Index, Section CH, Week 7844, Derwent Publications (GB), Class A, AN 78 79190a (& JP A 53 111 121) (1978).
- World Patent Index, Section CH, Week 7844, Derwent Publications (GB), Class A, AN 78-79190a (& JP-A-53 111 121) (1978).