Patents
US 5,380,683 A#7558094 Most CitedExpiredUnited States (USPTO)Utility

Ionized cluster beam deposition of sapphire and silicon layers

13Forward Citations (#7558094 Global)
0.4/yrCitation Velocity (#19199278 Global)
2.57Citation PageRank (#9740227 Global)
12Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Sapphire, a highly stable oxide of aluminum having the chemical formula of Al 2 O 3 , is placed in a crucible. The crucible is heated to vaporize the sapphire therein. The sapphire vapor is ejected through a nozzle in the crucible and into a region having a vacuum pressure of approximately 10 -5 Torr or less. As the vapor leaves the crucible through the nozzle, atom aggregates or clusters are formed through a supercooled phenomenon due to adiabatic expansion. The vacuum region has disposed therein a substrate of silicon. The sapphire vapor is accelerated towards the substrate where it deposits on a surface of the substrate in a uniformly distributed thin layer.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 12 · Forward citations: 13.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for forming a sapphire layer and a silicon layer superjacent a substrate, comprising the steps of: providing sapphire in a first crucible having a first nozzle; providing silicon in a second crucible having a second nozzle; positioning a substrate and said crucibles within a vacuum region, said vacuum region having a first pressure level; heating said first crucible to a first temperature to vaporize said sapphire at a second pressure level within said first crucible, said second pressure level being substantially greater than said first pressure level, such that said sapphire v

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • Applied Surface Science 33/34 (1988); Urban et al.; pp. 966 971; Optical Properties of Reactive ICB Aluminum Oxide Film Deposited on Si(100 J. Appl. Phys. 63(1) (Jan. 1, 1988); Hashimoto et al.; Optical and Structural Characteristics of AL 2 O 3 Films Deposited by the Reactive Ionized Cluster Beam M
  • Applied Surface Science 33/34 (1988); Urban et al.; pp. 966-971; "Optical Properties of Reactive ICB Aluminum Oxide Film Deposited on Si(100 J. Appl. Phys. 63(1) (Jan. 1, 1988); Hashimoto et al.; Optical and Structural Characteristics of AL2 O3 Films Deposited by the Reactive Ionized Cluster Beam Me
  • IEEE Transactions on Electron Devices 14(5); May 1987; Yamada et al.; "Metallization by Ionized Cluster Beam Deposition", pp. 1018-1025.
  • IEEE Transactions on Electron Devices 14(5); May 1987; Yamada et al.; Metallization by Ionized Cluster Beam Deposition , pp. 1018 1025.
  • J. Appl. Phys. 64(9) (Nov. 1, 1988); Yamada and Torii; pp. 4509 4515; Thin Heteroepitaxial Si ON Sapphire Films Grown at 600 C. by Reactive Beam Deposition .